Wood door leaf component, wood door leaf and manufacturing method of wood door leaf
A technology of a log door leaf component and a manufacturing method, which is applied in the production field of wooden doors and wooden doors, can solve problems such as damage, affecting the service life of the door, deformation, etc., and achieves the effect of ensuring integrity and improving service life.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0027] refer to Figure 1-3 , a method for making a log door leaf, comprising the steps of:
[0028] The first step: woodworking. First of all, the woodwork is processed into such as figure 1 The left and right door stand 1, 1', the upper and lower crosspieces 2, 2', the middle crosspiece 3, and the door blocking plate 4; the upper and lower crosspieces 2, 2', and the middle crosspiece 3 have not yet been provided with tenons or tenons or mortise joint holes.
[0029] Step Two: Paint. For each left and right door frame 1, 1 ', upper and lower crosspieces 2, 2 ', middle crosspiece 3, door blocking plate 4, paint respectively to obtain the log door leaf member. The paint can be a primer or a primer+finish paint or a waterproof paint.
[0030] The third step: assembly. After the paint in the second step is dried, tenon joint holes are opened on the upper and lower crosspieces 2, 2' and the middle crosspiece 3, and the upper and lower crosspieces 2, 2', the middle crosspiece...
Embodiment 2
[0034] refer to Figure 4 The difference between this embodiment and Embodiment 1 is that in the third step, a first tenon groove 7' is provided on the upper and lower crosspieces 2, 2' and the middle crosspiece 3, and the center of the first tenon groove 7' protrudes A first tenon 8'. The second tenon 8 provided on the inner side of the left and right vertical squares 1, 1', and the second tenon 8 is provided with a second tenon groove 7 in the center of the second tenon. Mortise the upper and lower crosspieces 2, 2', the middle crosspiece 3 with the left and right uprights 1, 1', where the first tenon groove 7' is tenoned with the second tenon head 8, and the second tenon groove 7 is connected with the first tenon head 8', through two groups of mortise joints, the upper and lower crosspieces 2, 2', the middle crosspiece 3, and the left and right uprights 1, 1' are more firmly connected.
[0035] The outer chamfers of the joints of the left and right uprights 1, 1', the upp...
Embodiment 3
[0037] refer to Figure 5 . A method for making a log door leaf, comprising the steps of:
[0038] The first step: woodworking. First of all, the woodwork is processed into such as figure 1 The left and right uprights 1, 1', the upper and lower crosspieces 2, 2', the middle crosspieces 3, and the door blocking plate 4 are shown; Tenon joint holes.
[0039] Step Two: Paint. For each left and right vertical frame 1,1 ', upper and lower crosspieces 2,2 ', middle crosspiece 3, door blocking plate 4, obtain the log door leaf component with the paint that primer and topcoat carry out respectively.
[0040] The third step: assembly. The left and right uprights 1, 1' can be cut according to the needs of on-site installation. Then the upper and lower crosspieces 2, 2' and the middle crosspiece 3 are provided with tenon joint holes, and the upper and lower crosspieces 2, 2', the middle crosspiece 3 are tenon-jointed with the left and right door frame 1, 1' through the tenon 5 to ...
PUM
Login to View More Abstract
Description
Claims
Application Information
Login to View More - R&D
- Intellectual Property
- Life Sciences
- Materials
- Tech Scout
- Unparalleled Data Quality
- Higher Quality Content
- 60% Fewer Hallucinations
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2025 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com