Electric tool cylinder lubricating grease and preparation method thereof
A technology for electric tools and grease, applied in the field of grease, can solve the problems of inability to meet high-frequency use requirements, low frequency of electric tools, long working hours, etc., to achieve low and long life, reduce energy loss, and prolong service life Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0037] With 837.8g high phenyl silicone oil (phenyl content 30%) (V 25℃ , 289mm 2 / s), 27.4g diphenylsilanediol is added to the reaction kettle, after heating until it is completely melted, the specific surface area is 380m 2 / g fumed silica 82.2g, keep for 20min, cool down to 80-100℃, add T53130g, Afton diesel engine oil compounding agent HiTEC8799B50g, mix and stir for 20min, set the gap to 5μm colloid grinding once, and then use the gap setting It is determined that the front 10μ / back 2μ three-roll mill grinds 1 time.
Embodiment 2
[0039] With 796.3g high phenyl silicone oil (phenyl content 40%) (V 25℃ , 321mm 2 / s), 27.4g diphenylsilanediol is added to the reaction kettle, and after heating to be completely melted, the specific surface area is 308m 2 / g fumed silica 96.5g, hold for 30min, cool down to 80-100℃, add T53142g, Afton diesel engine oil complex agent HiTEC8799B65.2g, mix and stir for 30min, set the gap to 5μm colloid grinding once, and then use The gap is set at the front 10μ / back 2μ with a three-roll grinder for one pass.
Embodiment 3
[0041] With 410g high phenyl silicone oil (phenyl content 30%) (V 25℃ , 289mm 2 / s), 96.5g lithium bentonite, and 30g ethanol aqueous solution (95%) of polar dispersant, heat and stir to volatilize the dispersant, continue heating to 135°C, and keep the temperature for 30 minutes, add the remaining 410g high phenyl Silicone oil is used to adjust the consistency of grease, the temperature is lowered to 80-100°C, additives T35143g and HiTEC8799B40.5g are added, and stirred for 20 minutes. Grind once with a colloid mill with a gap of 5 μ, then grind with a three-roll machine with a gap of 5 μ before / 2 μ behind, degas and pack to obtain the finished product.
PUM
| Property | Measurement | Unit |
|---|---|---|
| specific surface area | aaaaa | aaaaa |
| thermal decomposition temperature | aaaaa | aaaaa |
| thermal decomposition temperature | aaaaa | aaaaa |