A technology of hydroxypropyl starch ether and fluorite ore, which is applied in flotation, solid separation, etc., can solve the problem of difficult separation of fluorite, calcite and barite gangue minerals, low effective recovery rate, and poor quality of flotation concentrate Poor and other problems, achieve good suppression ability, improve grade and recovery rate, shorten the effect of flotation process
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0019] The flotation test is carried out by XFGⅡ hanging tank flotation machine. First, add 2g of fluorite or calcite or barite pure minerals to the flotation tank, then add 35ml of distilled water to stir and adjust the slurry, and use HCl or NaOH to adjust the pH of the slurry to 9. And stir, then add hydroxypropyl starch ether inhibitor 20mg / L and stir for 5min, sodium oleate 20mg / L, and then scrape bubbles. After the flotation test, the foam product is filtered, dried, weighed, assayed and the recovery rate calculated.
[0020] The test results of Example 1 are shown in Table 1.
[0021] Table 1 Test comparison results
[0022]
Embodiment 2
[0024] The flotation test is carried out by XFGⅡ hanging tank flotation machine. First, add 2g of fluorite or calcite or barite pure minerals to the flotation tank, then add 35ml of distilled water to stir and adjust the slurry, and use HCl or NaOH to adjust the pH of the slurry to 11. And stir, then add hydroxypropyl starch ether inhibitor 60mg / L and stir for 2min, sodium oleate 40mg / L, and then scrape bubbles. After the flotation test, the foam product is filtered, dried, weighed, assayed and the recovery rate calculated.
[0025] The test results of Example 2 are shown in Table 2.
[0026] Table 2 Test comparison results
[0027]
Embodiment 3
[0029] The flotation test was carried out with XFGⅡ type hanging tank flotation machine. First, 1g of fluorite and 1g of barite were added to the flotation tank, then 35ml of distilled water was added to stir the slurry, and the pH of the pulp was adjusted to 9 with HCl or NaOH and stirred, and then Add hydroxypropyl starch ether inhibitor 60mg / L and stir for 3min, sodium oleate 100mg / L in turn, then scrape bubbles again, artificially mix ore and separate by flotation once. After the flotation test, the foam product is filtered, dried, weighed, assayed and the recovery rate calculated.
[0030] Example 3 test results are shown in Table 3.
[0031] Table 3 test results
[0032] Inhibitor
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com