A technology of CO2 and shredded tobacco, applied in the field of tobacco, can solve the problems of loss of chemical composition of shredded tobacco, low rate of change of the whole shredding rate and high production cost, so as to widen the scope of use of raw materials, improve the rate of change of the shredded shredding rate, and enhance the use value of raw materials. Effect

Active Publication Date: 2018-10-02
CHINA TOBACCO HENAN IND
View PDF7 Cites 0 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

Its advantage is high filling capacity, reaching 6.5cm3 / g~7.3 cm3 / g, which can effectively remove miscellaneous gases in shredded tobacco, improve the product quality of cigarettes, and reduce the amount of tar in cigarette smoke; its disadvantage is that during the production process, the production of shredded tobacco Larger shreds, serious loss of some chemical components of shredded tobacco, more aroma loss, heavy burnt smell, dry smoke, 50% to 60% lower change rate of shredded shreds, high production cost, and carbonization of shredded tobacco during the production process, serious Sometimes it even catches fire and smokes

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0010] A medium-low temperature CO in shredded tobacco 2 The expansion process includes the following steps: ① immerse shredded tobacco with a moisture content of 19% in liquid CO 2 In the process, immerse for 100s to obtain dry ice cut tobacco; ② loosen the dry ice cut tobacco obtained in step ① (loosen by 40Hz loosening roller) and feed it into the HT steam expansion device (purchased from Qinhuangdao Tobacco Machinery Co., Ltd. ) for pre-expansion (after the material is loosened, the dry ice shredded tobacco flow rate is 1200kg / h, the steam flow rate is 100kg / h, the steam temperature is 155°C, and the pre-expansion time is 4 s); (purchased from Qinhuangdao Tobacco Machinery Co., Ltd.) for expansion drying (the moisture content of cut tobacco after expansion drying is 13.5%, and the filling value is 6.2 cm 3 / g), the flow rate of hot air entering the air dryer is 22m / s, and the temperature is 220°C.

[0011] The structural changes of the low-temperature expanded shredded t...

Embodiment 2

[0020] A medium-low temperature CO in shredded tobacco 2 The expansion process includes the following steps: ① immerse shredded tobacco with a moisture content of 18% in liquid CO 2 , dipped for 60s to obtain dry ice shredded tobacco; ② loosen the dry ice shredded tobacco obtained in step ① (loosen by a 40Hz loosening roller) and feed it into the HT steam expansion device (purchased from Qinhuangdao Tobacco Machinery Co., Ltd. ) for pre-expansion (after the material is loosened, the dry ice shredded tobacco flow rate is 1200kg / h, the steam flow rate is 100kg / h, the steam temperature is 150°C, and the pre-expansion time is 5 s); (purchased from Qinhuangdao Tobacco Machinery Co., Ltd.) for expansion drying (the moisture content of cut tobacco after expansion drying is 14.5%, and the filling value is 5.7 cm 3 / g), the flow rate of hot air entering the air dryer is 21m / s, and the temperature is 200°C.

Embodiment 3

[0022] A medium-low temperature CO in shredded tobacco 2 The expansion process includes the following steps: ① immerse shredded tobacco with a moisture content of 20% in liquid CO 2 , dipped for 80s to obtain dry ice shredded tobacco; ② loosen the dry ice shredded tobacco obtained in step ① (loosen by a 40Hz loosening roller) and feed it into the HT steam expansion device (purchased from Qinhuangdao Tobacco Machinery Co., Ltd. ) for pre-expansion (after the material is loosened, the dry ice shredded tobacco flow rate is 1200kg / h, the steam flow rate is 100kg / h, the steam temperature is 160°C, and the pre-expansion time is 4 s); (purchased from Qinhuangdao Tobacco Machinery Co., Ltd.) for expansion drying (the moisture content of cut tobacco after expansion drying is 12.5%, and the filling value is 6.4 cm 3 / g), the flow rate of hot air entering the air dryer is 23m / s, and the temperature is 200°C.

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

PUM

No PUM Login to view more

Abstract

The invention belongs to a low-temperature CO2 expansion process for shredded tobacco, comprising the following steps: ① immerse shredded tobacco with a moisture content of 18% to 20% in liquid CO2 for 60 to 100 seconds to obtain shredded tobacco with dry ice; ② immerse shredded tobacco with dry ice obtained in step ① After the shredded tobacco is loose, it enters the HT steam expansion device through quantitative feeding for pre-expansion; ③The pre-expanded shredded tobacco is sent to the air dryer for expansion and drying, and the flow rate of the hot air entering the air dryer is 21m / s~23m / s , The temperature is 200 ℃ ~ 230 ℃. Adopting the process of the present invention reduces the treatment intensity of the carbon dioxide process, reduces the fragmentation during the expansion process, improves the whole cut rate of the expanded cut tobacco, and the whole cut rate is 74% to 78%, reduces the broken shred rate, and the broken shred rate is 1.4% to 2.1%, Improve the change rate of the whole yarn rate, and the change rate of the whole yarn rate is 73% to 77%.

Description

technical field [0001] The invention relates to the field of tobacco, in particular to a medium-low temperature CO 2 The expansion process is mainly used in the processing of shredded leaf in cigarette enterprises. Background technique [0002] During the current cigarette production process, CO 2 Cut tobacco expansion technology is the most mature and popular. Its main steps are: the tobacco leaves are subjected to vacuum re-moisture, loose re-moisture, mixed pre-storage and shredded tobacco leaves to obtain shredded leaves with a water content of 22% to 24%. 2 Dipping for a certain period of time (60s) to form dry ice shreds. After being loosened, they are then heated instantaneously by hot air at a high speed of 27m / s to 31m / s at a high temperature of 320°C to 350°C. The shredded leaves are fully expanded and made into shredded leaves with a moisture content of 6% to 8%. After regaining moisture, the moisture content reaches the requirement of 12.7% to 13.8%, which is s...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

Application Information

Patent Timeline
no application Login to view more
Patent Type & Authority Patents(China)
IPC IPC(8): A24B3/18
CPCA24B3/185
Inventor 张月华郜海民熊安言张爱忠高尊华王根发郭华诚许淑红吴艳艳张文海杨耀伟王雷李传奇张健
Owner CHINA TOBACCO HENAN IND
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Try Eureka
PatSnap group products