Lithium ion battery aluminum plastic film damage detecting method
A lithium-ion battery and damage detection technology, which is applied in the direction of chemical reaction of materials and material analysis by observing the influence of chemical indicators. It can solve problems such as difficulty in ensuring battery quality and verifying aluminum-plastic films. To achieve the effect of convenient detection, low cost, and ensure the quality of the battery
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0013] Embodiment 1: A method for detecting damage to an aluminum-plastic film of a lithium-ion battery, comprising the following steps:
[0014] 1) preparation detection solution: the copper chloride that is 0.5% by weight, the ethanol that is 9% by weight, the n-butanol that is 0.3% by weight, the sodium dodecylbenzenesulfonate that is 0.4% by weight 1.8% by weight of polyacrylamide and 88% by weight of water are mixed to prepare a detection solution;
[0015] 2) Inspection: Put the aluminum-plastic film to be tested into the test solution prepared in step 1) and soak for 2 minutes, and then observe the changes on the surface of the aluminum-plastic film. If there is reddish-brown copper precipitation on the surface of the aluminum-plastic film, then judge The aluminum-plastic film is damaged; if there is no change on the surface of the aluminum-plastic film, it is determined that the aluminum-plastic film is not damaged.
Embodiment 2
[0017] 1) Preparation detection solution: the copper chloride that is 1% by weight, the ethanol that is 10% by weight, the n-butanol that is 0.4% by weight, the sodium dodecylbenzenesulfonate that is 0.6% by weight , 2% by weight of polyacrylamide and 86% by weight of water are mixed to prepare a detection solution;
[0018] 2) Inspection: Soak the aluminum-plastic film to be tested in the test solution prepared in step 1) for 1 minute, and then observe the changes on the surface of the aluminum-plastic film. The aluminum-plastic film is damaged; if there is no change on the surface of the aluminum-plastic film, it is determined that the aluminum-plastic film is not damaged.
Embodiment 3
[0020] 1) preparation detection solution: the copper chloride that is 1.5% by weight, the ethanol that is 11% by weight, the n-butanol that is 0.5% by weight, the sodium dodecylbenzene sulfonate that is 0.6% by weight , 2.4% by weight of polyacrylamide and 84% by weight of water are mixed to prepare a detection solution;
[0021] 2) Inspection: Put the aluminum-plastic film to be tested into the test solution prepared in step 1) and soak for 0.5min, and then observe the changes on the surface of the aluminum-plastic film. If there is reddish-brown copper precipitation on the surface of the aluminum-plastic film, then It is determined that the aluminum-plastic film is damaged; if there is no change on the surface of the aluminum-plastic film, it is determined that the aluminum-plastic film is not damaged.
[0022] The working principle of the present invention: since the main component polypropylene of the CPP / PPA layer of the aluminum-plastic film is a non-polar molecule, its ...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com