Biological filler and preparation method thereof
A technology of biological filler and magnesium oxide, applied in the field of water treatment, can solve problems such as instability, cure the symptoms but not the root cause, and achieve the effect of strong biophilicity, accelerated growth and good film-hanging effect.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
preparation example Construction
[0027] See figure 1 , the present invention also provides a preparation method of biological filler, comprising the following steps:
[0028] S1. Mix the components of the above-mentioned biological filler evenly;
[0029] S2. Using an injection molding machine for injection molding to obtain a biological filler.
[0030] The biological filler prepared in step S2 may be in the shape of a spherical shape, a sheet shape, or the like.
Embodiment approach 1
[0032] The invention provides a biological filler, comprising the following components: polyethylene, polypropylene, magnesium oxide, calcium oxide, potassium oxide;
[0033] The mass ratio of each component in the biological filler is: polyethylene 10%, polypropylene 60%, magnesium oxide, calcium oxide, potassium oxide 30% in total.
[0034] Further, the mass ratios of magnesium oxide, calcium oxide and potassium oxide in the biological filler are equal.
[0035] The present invention also provides a preparation method of biological filler, comprising the following steps:
[0036] S1. Mix the components of the above-mentioned biological filler evenly;
[0037] S2. Using an injection molding machine for injection molding to obtain a biological filler.
[0038] The biological filler prepared in step S2 may be in the shape of a spherical shape, a sheet shape, or the like.
Embodiment approach 2
[0040] The invention provides a biological filler, comprising the following components: polyethylene, polypropylene, magnesium oxide, calcium oxide, potassium oxide;
[0041] The mass ratio of each component in the biological filler is: polyethylene 5%, polypropylene 65%, magnesium oxide, calcium oxide, potassium oxide 30% in total.
[0042] Further, the mass ratios of magnesium oxide, calcium oxide and potassium oxide in the biological filler are equal.
[0043] The present invention also provides a preparation method of biological filler, comprising the following steps:
[0044] S1. Mix the components of the above-mentioned biological filler evenly;
[0045] S2. Using an injection molding machine for injection molding to obtain a biological filler.
[0046] The biological filler prepared in step S2 may be in the shape of a spherical shape, a sheet shape, or the like.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com