Formula and production method of easy-defoaming selenium plastic paint
A technology of resin and propylene glycol, which is applied in polyester coatings, coatings, etc., can solve the problems of poor defoaming of selenium plastic paints, and achieve the effect of preventing construction and ensuring rapidity
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment Construction
[0010] 30 kg of dehydrated malic acid resin, 10 kg of propylene glycol, 0.01 kg of polyethylene glycol (600), 1 kg of ultrafine silicon dioxide, 2 kg of polyamide wax (n-butanol, naphtha mixture), 1250 mesh of talcum powder 2 kg, 15 kg of o-phthalic unsaturated polyester resin, 0.1 kg of polyvinyl butyral, 10 kg of styrene, and 2 kg of selenium photoplastic initiator (D1173). Acid resin polymer (solid content 80%), propylene glycol, polyethylene glycol (600), ultrafine silicon dioxide, polyamide wax (n-butanol, petroleum naphtha mixture), talcum powder 1250 mesh, and continue to stir for 90 minutes , then add o-phthalic unsaturated polyester resin, polyvinyl butyral, styrene, defoaming polysiloxane and polyethylene glycol hydrophobic solid mixture, continue to stir for 30 minutes, and finally add selenium photoplastic initiator (D1173), avoid light.
PUM
Login to View More Abstract
Description
Claims
Application Information
Login to View More