A kind of oilfield ternary compound flooding oily sewage pretreatment agent and its treatment method
A ternary compound and pretreatment agent technology, which is applied in water/sewage treatment, water/sewage multi-stage treatment, biological water/sewage treatment, etc., can solve the problem of slow separation of sludge and water, difficulty in agglomeration, and deterioration of water quality, etc. To improve the economic and social benefits of the oil field, the system structure is simple and reasonable, and the process operation is stable
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0028] An oilfield three-element compound flooding oily sewage pretreatment agent, which includes the following raw materials by mass percentage: 10% of activated carbon, 30% of bentonite, 30% of zeolite powder, 6% of aluminum sulfate, 10% of polyferric sulfate, and 4% of acetone oxime %, ferrous sulfate 10%.
[0029] In the above formula, the zeolite powder is made of the following raw materials by mass percentage: 10% silicon dioxide, 35% aluminum oxide, 5% shell, 12% construction waste, 18% clay, and 20% adhesive; The agent is made of water glass and sodium carboxymethyl cellulose in a ratio of 30%:70%. The bentonite is 300 mesh calcium-based bentonite.
[0030] The treatment method for the oily sewage of the above oilfield ASP flooding includes the following steps:
[0031] 1) The oily wastewater from ASP flooding in the oil field is transported through pipelines to the primary sedimentation tank for natural sedimentation, and the sedimentation time is 24 hours to obtain...
Embodiment 2
[0039]An oily three-element compound flooding oily sewage pretreatment agent, which comprises the following raw materials by mass percentage: activated carbon 15%, bentonite 35%, zeolite powder 20%, aluminum sulfate 8%, polyferric sulfate 11%, acetone oxime 3 %, ferrous sulfate 8%.
[0040] In the above formula, the zeolite powder is made of the following raw materials by mass percentage: 20% silicon dioxide, 25% aluminum oxide, 10% shell, 15% construction waste, 15% clay, and 15% adhesive; The agent is made of water glass and sodium carboxymethyl cellulose in a ratio of 30%:70%. Bentonite is 500 mesh sodium bentonite.
[0041] The treatment method for the oily sewage of the above oilfield ASP flooding includes the following steps:
[0042] 1) The oily wastewater from ASP flooding in the oilfield is transported through pipelines to the primary sedimentation tank for natural sedimentation, and the sedimentation time is 12 hours to obtain the first supernatant;
[0043] 2) Th...
Embodiment 3
[0050] An oilfield three-element compound flooding oily sewage pretreatment agent, which includes the following raw materials by mass percentage: 20% of activated carbon, 15% of bentonite, 40% of zeolite powder, 8% of aluminum sulfate, 8% of polyferric sulfate, and 4% of acetone oxime %, ferrous sulfate 5%.
[0051] In the above formula, the zeolite powder is made of the following raw materials by mass percentage: 20% silicon dioxide, 25% aluminum oxide, 10% shell, 15% construction waste, 15% clay, and 15% adhesive; The agent is made of water glass and sodium carboxymethyl cellulose in a ratio of 30%:70%. Bentonite is 200 mesh acid bentonite.
[0052] The treatment method for the oily sewage of the above oilfield ASP flooding includes the following steps:
[0053] 1) The oily wastewater from ASP flooding in the oil field is transported through pipelines to the primary sedimentation tank for natural sedimentation, and the sedimentation time is 48 hours to obtain the first sup...
PUM