Urban road pavement grouting reinforcement construction method
A technology of road pavement and construction method, which is applied in the field of urban road pavement grouting reinforcement construction, can solve problems such as economic loss, large construction waste, and large traffic interference, and achieve the effect of enhancing strength
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0021] The urban road pavement grouting reinforcement construction method provided in this embodiment comprises the following steps:
[0022] (1) Investigate the fixed plate, visually observe the looseness of the staggered plate and the crack plate when the heavy vehicle passes through the road, and then determine the mud plate according to the situation of the plate crack when the vehicle passes after the rain;
[0023] (2) Arrange 5-7 grouting holes on the pumping plate, and the arranged grouting holes are distributed in a plum blossom shape. One grouting hole is drilled in the center of the pumping plate, and the rest of the grouting holes are selected around the pumping plate. At 50cm from the edge of the mud plate, the diameter of the drilled grouting hole is controlled at 5-8cm, and the drilling depth of the grouting hole is controlled at 5-8cm below the bottom of the mud plate;
[0024] (3) To prepare slurry, select 100 parts of Portland cement, 60 parts of fly ash and ...
Embodiment 2
[0029] This embodiment is basically the same as Example 1, except that the composition of the slurry is changed, and the slurry includes 90 parts by weight of Portland cement, 50 parts of fly ash, and 12 parts of concrete accelerator. parts, 30 parts of filler powder, 0.2 parts of aluminum powder, 4 parts of expansion agent, 1 part of defoamer and 60 parts of water.
Embodiment 3
[0031] This embodiment is basically the same as Example 1, except that the composition of the slurry is changed, and the slurry includes 110 parts by weight of Portland cement, 70 parts of fly ash, and 20 parts of concrete accelerator. parts, 48 parts of filler powder, 0.3 parts of aluminum powder, 8 parts of expansion agent, 3 parts of defoamer and 80 parts of water.
[0032] The filler powder in above-mentioned embodiment 1-3 comprises hematite, kaolinite, marble and granite, and the proportioning of hematite, kaolinite, marble and granite is 3:2:0.5:0.5, and described filler powder The preparation method comprises: a. pulverizing and pulverizing hematite, kaolinite, marble and granite through a 100-mesh sieve; b. uniformly mixing pulverized and pulverized hematite, kaolinite, marble and granite.
PUM

Abstract
Description
Claims
Application Information

- Generate Ideas
- Intellectual Property
- Life Sciences
- Materials
- Tech Scout
- Unparalleled Data Quality
- Higher Quality Content
- 60% Fewer Hallucinations
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2025 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com