Preparation process of fabric with one-way moisture guide function
A technology of one-way wetting and preparation process, applied in the field of knitted fabric manufacturing, can solve the problems of complex production process, high dosage of auxiliary agents and high production cost, and achieve the effects of avoiding raw material waste, reducing production cost and reducing dosage.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0025] Embodiment 1: A kind of preparation technology of fabric with unidirectional moisture-wicking function, comprises the following steps:
[0026] (1) 190G / M of 32 / 1FC+20D SPANDEX 2 Put the frame jersey fabric into the dyeing vat, treat it with 5g / l QH15 soft oil at 45°C for 12 minutes, and then dry it on a tenter chain dryer at 135°C;
[0027] (2) The waterproofing agent is formed into a micron-level linear water mist through the spraying device, and is sprayed on the inner surface layer of the cloth at a high speed to form a uniform waterproofing layer; the liquid-carrying rate of the waterproofing agent on the cloth is 25%;
[0028] (3) The fabric sprayed with a waterproof layer on one side is subjected to tenter heat setting, cooling, and pendulum or roll fall in sequence at a machine speed of 20 M / min.
[0029] Further, in order to improve the uniformity of spraying of the waterproofing agent on the cloth, the spraying device described in step (2) includes a silo 1, ...
Embodiment 2
[0038] (1) 200G / M of 100D / 48F POLYESTER+40S / 1 FC 2 Put the cotton-covered silk plain knitted fabric into the dyeing vat, treat it with 8g / l QH15 soft oil at 35°C for 5 minutes, and then dry it on a tenter type needle chain dryer at 125°C;
[0039] (2) The waterproofing agent is formed into a micron-level linear water mist through the spraying device, and is sprayed on the inner surface layer of the cloth at a high speed to form a uniform waterproofing layer; the liquid-carrying rate of the waterproofing agent on the cloth is 22%;
[0040] (3) The fabric sprayed with a waterproof layer on one side is subjected to tenter heat setting, cooling, and pendulum or roll fall in sequence at a machine speed of 15 M / min.
[0041] Further, in order to improve the spraying uniformity of the waterproofing agent on the cloth, the spraying device described in step (2) includes a silo, a group of spray heads, a centrifugal cutting disc and a return chute, and the spray head is installed at the...
Embodiment 3
[0051] (1) Will: 275G / M of 80D / 156F SD POLYESTERE (50D / 144F DTY / 30D / 12F HS FDY) 2 Put the double-sided knitted fabric into the dyeing vat, treat it with 10g / l QH15 soft oil at 55°C for 15 minutes, and then dry it on a stenter needle chain dryer at 140°C;
[0052] (2) The waterproofing agent is formed into a micron-level linear water mist through the spraying device, and is sprayed on the inner surface layer of the cloth at a high speed to form a uniform waterproofing layer; the liquid-carrying rate of the waterproofing agent on the cloth is 30%;
[0053] (3) The fabric sprayed with a waterproof layer on one side is subjected to tenter heat setting, cooling, and pendulum or roll fall in sequence at a machine speed of 18 M / min.
[0054] In order to improve the spraying uniformity of the waterproofing agent on the cloth, the spraying device described in step (2) includes a silo, a group of spray heads, a centrifugal cutting disc and a return trough, and the spray heads are instal...
PUM