Embodiment 1
[0022] Step 1. For the selection of yarn count, the warp yarn is 9.5tex, and the cotton combed strands with Xinjiang long-staple cotton content accounting for 64% are selected. The single strength of the yarn should be high: long-staple cotton and fine Blended compact spinning of velvet cotton, blending ratio: 30% long-staple cotton and 70% fine-staple cotton are selected for blending, and the weft direction is a 16S and a 7S double-ply yarn alternately;
[0023] Step 2, singeing the yarn, burning off the hairiness on the surface of the yarn by means of a high-temperature flame;
[0024] Step 3, impregnating the softened sericin, and doing a good job of moisture-proofing;
[0025] Step 4. Draw warp yarns of a certain number and length from the winding bobbin to form a piece of yarn, so that the warp yarns have uniform tension, and are tightly wound on the warp beam parallel to each other to form a weaving beam. preliminary preparation;
[0026] Step 5, threading the warp yar...
Embodiment 2
[0031] Step 1. For the selection of yarn count, the warp yarn is 9.3tex, and the cotton combed strands with Xinjiang long-staple cotton content accounting for 78% are selected. Cotton blended compact spinning, blending ratio: 30% long-staple cotton and 70% fine-staple cotton are selected for blending, and the weft direction is a 16S and a 7S double-ply yarn alternately;
[0032] Step 2, singeing the yarn, burning off the hairiness on the surface of the yarn by means of a high-temperature flame;
[0033] Step 3, impregnating the softened sericin, and doing a good job of moisture-proofing;
[0034] Step 4. Draw warp yarns of a certain number and length from the winding bobbin to form a piece of yarn, so that the warp yarns have uniform tension, and are tightly wound on the warp beam parallel to each other to form a weaving beam. preliminary preparation;
[0035] Step 5, threading the warp yarns into the heald eyes and reed teeth is to further temporarily and partially fix the ...
Embodiment 3
[0040] Step 1. For the selection of yarn count, the warp yarn is 9.1tex, and the cotton combed strands with Xinjiang long-staple cotton content accounting for 80% are selected. Cotton blended compact spinning, blending ratio: 30% long-staple cotton and 70% fine-staple cotton are selected for blending, and the weft direction is a 16S and a 7S double-ply yarn alternately;
[0041] Step 2, singeing the yarn, burning off the hairiness on the surface of the yarn by means of a high-temperature flame;
[0042]Step 3, impregnating the softened sericin, and doing a good job of moisture-proofing;
[0043] Step 4. Draw warp yarns of a certain number and length from the winding bobbin to form a piece of yarn, so that the warp yarns have uniform tension, and are tightly wound on the warp beam parallel to each other to form a weaving beam. preliminary preparation;
[0044] Step 5, threading the warp yarns into the heald eyes and reed teeth is to further temporarily and partially fix the w...
PUM
Property | Measurement | Unit |
---|---|---|
width | aaaaa | aaaaa |
length | aaaaa | aaaaa |
length | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com