Production method for secure sliding window resistant to deformation
A production method and technology for sliding windows, applied in the direction of metal material coating process, etc., can solve the problems of poor machining accuracy, easy deformation, insufficient strength, etc., and achieve the effects of improving machining accuracy, reducing easy deformation, and making up for insufficient strength.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0032] A method for producing a safe and anti-deformation sliding window, the steps of which are as follows:
[0033] (1) Decompose the required sliding window frame base parts according to the size of the design drawings, use a laser cutting machine to make the window frame base parts and use screws to assemble and weld the window frame;
[0034] (2) Cutting, bending and stamping according to the design drawings to make sliding window base parts and edge banding strips;
[0035] (3) After the assembly and welding, the window frame and the base parts of the sliding window are put into the colloid pool for 15 minutes, and the temperature is controlled at 22°C. The pH value of the foaming agent is 10 in the alkaline cleaning agent for 5 minutes to carry out degreasing treatment;
[0036] (4) Put the window frame and sliding window base parts in the step (3) into the pickling pool equipped with pickling solution, pickle at normal temperature for 5 minutes, put them into the tank...
Embodiment 2
[0041] A method for producing a safe and anti-deformation sliding window, the steps of which are as follows:
[0042] (1) Decompose the required sliding window frame base parts according to the size of the design drawings, use a laser cutting machine to make the window frame base parts and use screws to assemble and weld the window frame;
[0043] (2) Cutting, bending and stamping according to the design drawings to make sliding window base parts and edge banding strips;
[0044] (3) After the assembly and welding, the window frame and sliding window base parts are put into the colloid pool for 35 minutes, the temperature is controlled at 20°C, and the edge banding strip is put into a mixture of inorganic low-alkaline additives, surfactants, and disinfectants. The pH value of the foaming agent is 12 in the alkaline cleaning agent for 8 minutes to carry out degreasing treatment;
[0045] (4) Put the window frame and the sliding window base part in the step (3) into the picklin...
Embodiment 3
[0050] A method for producing a safe and anti-deformation sliding window, the steps of which are as follows:
[0051] (1) Decompose the required sliding window frame base parts according to the size of the design drawings, use a laser cutting machine to make the window frame base parts and use screws to assemble and weld the window frame;
[0052] (2) Cutting, bending and stamping according to the design drawings to make sliding window base parts and edge banding strips;
[0053](3) After the assembly and welding, the window frame and sliding window base parts are put into the colloidal pool for 20 minutes, and the temperature is controlled at 21°C. The pH value of the foaming agent is 11 in the alkaline cleaning agent for 7 minutes to carry out degreasing treatment;
[0054] (4) Put the window frame and sliding window base parts in the step (3) into the pickling tank equipped with pickling solution, pickle for 8 minutes at normal temperature, put them into the tank with phos...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com