A technology of glucose oxidase and polymer materials, which is applied in the field of polymer materials carrying glucose oxidase and its preparation, can solve the problems of difficulty in effectively exerting curative effect, poor selectivity, and poor stability, and achieve excellent biocompatibility , maintaining the activity of biological enzymes, and the effect of high-efficiency delivery
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0046] A polymer carrier with enzyme protection, including folic acid and zinc chloride to form a complex template. The polymer of this embodiment is prepared by the following method:
[0047] (1) Get 2mL concentration of 2mM folic acid (FA) into a 10mL beaker, add 1mL concentration of 2wt% polyvinyl alcohol (PVA), then throw 50 μL glucose oxidase (GOx), add 500mL zinc chloride under stirring at room temperature, The final volume of the system was 4 mL, and the mixed solution was obtained by ultrasonication for 5 min.
[0048](2) Add 400 mL of Tris solution (pH=8.0) with a concentration of 0.1M to the solution obtained in step (1), adjust the pH value to about 7.6, and then add 400 μL of dopamine (DA) with a concentration of 5 mg / mL to the mixed solution Stir for 48 hours, centrifuge, and redissolve to obtain polydopamine nanoparticles with metal frameworks loaded with enzymes, which are denoted as NCPs / GOx@PDA NPs.
Embodiment 2
[0050] A polymer carrier with enzyme protection function, including dissociating a ligand template to obtain polydopamine nanoparticles. The polymer of this embodiment is prepared by the following method:
[0051] (1) Get 2mL concentration of 2mM folic acid (FA) into a 10mL beaker, add 1mL concentration of 2wt% polyvinyl alcohol (PVA), then drop into 50 μL glucose oxidase (GOx), add 500mL zinc chloride under stirring at room temperature, The final volume of the system was 4 mL, and the mixed solution was obtained by ultrasonication for 5 min.
[0052] (2) Add 400 mL of Tris solution (pH=8.0) with a concentration of 0.1M to the solution obtained in step (1), adjust the pH value to about 7.6, and then add 400 μL of dopamine (DA) with a concentration of 5 mg / mL to the mixed solution Stir for 48 hours, centrifuge and dialyze with 10 mM phosphate buffer (pH=7.4) for 1 hour, centrifuge and redissolve to obtain GOx@PDA NPs.
Embodiment 3
[0054] A polymer carrier with enzyme protection function, including dissociating a ligand template to obtain polydopamine nanoparticles. The polymer of this embodiment is prepared by the following method:
PUM
Property | Measurement | Unit |
---|---|---|
Particle size | aaaaa | aaaaa |
Particle size | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com