Formaldehyde-free melamine retanning agent, preparation method and equipment
A formaldehyde melamine, retanning agent technology, applied in small raw hide/large raw hide/leather/fur treatment, tanning treatment, small raw hide/large raw hide/leather hide/fur chemical treatment, etc., can solve problems such as the harm of leather products
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
preparation example Construction
[0031] Adopt the preparation method of a kind of formaldehyde-free melamine retanning agent as described above, comprise the steps:
[0032] S101: mixing starch, water, and periodic acid in parts by weight and then stirring to obtain a mixed solution;
[0033] S102: adjust the pH of the mixed solution to 1.8-2 in the follow-up reaction vessel, raise the temperature to 30-40° C. and react for 5-8 hours to prepare a polyaldehyde compound solution;
[0034] S103: Adjust the pH of the polyaldehyde compound solution to 9-10, raise the temperature to 80-90° C., add the amino compound in parts by weight, and stir again until the reaction is complete;
[0035] S104: After the reaction is complete, lower the temperature to 70°C, adjust the pH to 4-5, add leveling agent in parts by weight, and let it stand for 2 hours to prepare a formaldehyde-free melamine retanning agent.
[0036] Further, the amino compound is a polymer of 50-60 parts of urea and 20-30 parts of melamine.
[0037] F...
specific Embodiment
[0053] 300g of starch, 650g of water, and 2g of periodic acid are put into the mixing tank 10 in parts by weight and are stirred and mixed evenly by the first stirring unit 11, and then sent to the adjusting tank 20; , the heating plate 23 is heated to 40° C. for 5 hours to react to prepare a polyaldehyde compound solution; again, the acid-base regulator 21 is used to adjust the pH of the polyaldehyde compound solution to 9.5 by adding sodium hydroxide, and the heating plate 23 is used to Raise the temperature to 86°C, add 50g of urea and 30g of melamine in parts by weight, and start the second stirring unit 24 until the reaction is complete; Add acetic acid to adjust the pH to 5 and add 12g of leveling agent. After standing for 2 hours, about 1014g of formaldehyde-free melamine retanning agent can be obtained.
PUM