Leather flatting coating composition and preparation method thereof
A matting coating and composition technology, applied in fiber treatment, textiles and papermaking, etc., can solve the problems of not showing the original color of leather, insufficient matting degree, poor transparency, etc., and achieve high matting degree, good hand feeling and long-lasting effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0018] Example 1. Take 5% by weight of dimethylformamide, 10% of methyl ethyl ketone, 20% of butyl acetate, 6% of ethyl acetate, 50% of polyurethane resin, and silica 6 as a matting agent with a particle diameter of 1.2μm. %, dispersant methyl amyl alcohol 1%, slippery feel agent LA-322 1%, vehicle PT-4235 1%. The method for preparing the above matting coating composition is:
[0019] ①Put dimethylformamide, methyl ethyl ketone, ethyl acetate, and butyl acetate into the dispersion tank, then add the polyurethane resin, stir evenly, so that the polyurethane resin is completely dissolved;
[0020] ②While the mixture is constantly stirred, slowly add the matting agent and keep stirring for 60 to 90 minutes to make it evenly dispersed in the system;
[0021] ③While stirring, add the hand-feeling agent, dispersant, coloring agent, and thickening agent in sequence, and continue to stir for 30 to 60 minutes to obtain slippery matte paint.
Embodiment 2
[0022] Example 2, Take 3% dimethylformamide, 13% methyl ethyl ketone, 20% butyl acetate, 14% ethyl acetate, 42% polyurethane resin, and a matting agent silica 4 with a particle diameter of 1.4μm in weight ratio. %, dispersant methyl pentanol 1%, cyanohydroxycellulose ethyl vinyl vinculin thickener 1%, vehicle MG-C 1%, astringent feel agent HM-4930 1%, the preparation method of the above embodiment As described in Example 1, the astringent matting paint can be obtained.
Embodiment 3
[0023] Example 3 Take 4% dimethylformamide, 10% methyl ethyl ketone, 25% butyl acetate, 11.3% ethyl acetate, 43% polyurethane resin, and a matting agent silica 5 with a particle diameter of 1.6μm in weight ratio. %, dispersant polyacrylamide 1.2%, vehicle PT-4235 1.2%, oily feel agent LA-351 1.3%, the preparation method of the above embodiment is as described in Example 1 to obtain an oily matte coating.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com