Leather flatting coating composition and preparation method thereof
A matte coating and composition technology, applied in fiber treatment, textiles and papermaking, etc., can solve the problems of inability to show the original color of leather, insufficient matting, good transparency, etc., and achieve high matting, good hand feel, and good transparency. Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0018] Embodiment 1, get dimethyl formamide 5% by weight, butanone 10%, butyl acetate 20%, ethyl acetate 6%, polyurethane resin 50%, particle diameter is the matting agent silicon dioxide 6 of 1.2 μm %, dispersant methyl amyl alcohol 1%, slip agent LA-322 1%, vehicle PT-4235 1%. The method for preparing above-mentioned matting coating composition is:
[0019] ① Add dimethylformamide, butanone, ethyl acetate, and butyl acetate into the dispersion tank, then add polyurethane resin, stir evenly, and completely dissolve the polyurethane resin;
[0020] ②Under constant stirring of the mixture, slowly add the matting agent and keep stirring for 60-90 minutes to make it evenly dispersed in the system;
[0021] ③Under stirring, add hand feeling agent, dispersant, vehicle and thickener in sequence, and continue stirring for 30-60 minutes to obtain slippery matte coating.
Embodiment 2
[0022] Embodiment 2, get dimethylformamide 3% by weight, butanone 13%, butyl acetate 20%, ethyl acetate 14%, polyurethane resin 42%, particle diameter is the matting agent silicon dioxide 4 of 1.4 μm %, dispersant methyl amyl alcohol 1%, cyanhydroxycellulose ethyl cellulose thickener 1%, vehicle MG-C 1%, astringent feel agent HM-4930 1%, the preparation method of the above-mentioned examples As described in Example 1, the astringent matting paint can be obtained.
Embodiment 3
[0023] Embodiment 3, get dimethylformamide 4% by weight, methyl ethyl ketone 10%, butyl acetate 25%, ethyl acetate 11.3%, polyurethane resin 43%, particle diameter is the matting agent silica 5 of 1.6 μm %, dispersant polyacrylamide 1.2%, vehicle PT-4235 1.2%, oily feel agent LA-351 1.3%, the preparation method of the above-mentioned examples is as described in Example 1 to obtain the oily matte coating.