Unlock instant, AI-driven research and patent intelligence for your innovation.

Method for manufacturing waterproof soft-surface leather

A production method and leather technology, applied in leather impregnation, leather surface treatment, small raw hide/big raw hide/leather/fur treatment, etc., can solve the problem of low waterproof performance, achieve outstanding waterproof effect, avoid wrinkles, and enhance toughness Effect

Inactive Publication Date: 2014-02-26
JIHUA 3515 LEATHER & SHOES
View PDF3 Cites 1 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

At present, most of the painted waterproof leathers on the market are only waterproof in the static state, and the waterproof performance is not high; the dynamic waterproof leather is limited to unpainted suede or split leather, and the production method is simple, without considering the possible production during the process. Quality problems and operation conditions such as loose noodles, fried noodles, pulping, process cleaning, etc. The product is also limited by variety when used in shoemaking, and can only be applied to certain varieties such as casual shoes and sports shoes.

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Image

Smart Image Click on the blue labels to locate them in the text.
Viewing Examples
Smart Image
  • Method for manufacturing waterproof soft-surface leather

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0030] Embodiment 1: the manufacture method of waterproof soft leather: comprise the following steps:

[0031] A: Waterproof treatment: ①. Squeeze the wet blue leather, shave it evenly, rewet, retan, and dye it; ②. Add 0.1% of the waterproof material baking soda and 0.1% of the weight of the leather to the leather treated in step ①. 1% polyacrylic acid derivative Jintan PA-11 is tuned in the drum pH When the value reaches 4, add Jintanquor S I (Taiwan Fuying) which accounts for 8% of the weight of the leather, and after turning for 60 minutes, add Zonyl 602, which accounts for 3% of the weight of the leather, and then add 1.2% formic acid to adjust pH When the value reaches 2.5, wash with water, change the bath, and adjust with formic acid pH When the value reaches 2.5, add 3% of leather weight Metal salt chromium powder, rotated for 60 minutes, washed with water, drummed, squeezed and stretched, vacuum dried, re-moisturized and softened to obtain waterproof leather;

[00...

Embodiment 2

[0033] Embodiment 2: the manufacture method of waterproof soft leather: comprise the following steps:

[0034]A: Waterproof treatment: ①. Squeeze the wet blue leather, shave it evenly, rewet, retan, and dye it; ②. Add 0.1% of the waterproof material baking soda and 0.1% of the weight of the leather to the leather treated in step ①. 1% polyacrylic acid derivative Jintan PA-11 is tuned in the drum pH When the value reaches 4, add Jintanquor S I (Taiwan Fuying) which accounts for 8% of the weight of the leather, and after turning for 60 minutes, add Zonyl 602, which accounts for 3% of the weight of the leather, and then add 1.2% formic acid to adjust When the pH value reaches 2.5, wash with water, change the bath, and adjust with formic acid. pH When the value reaches 2.5, add 3% of leather weight Metal salt chromium powder, rotated for 60 minutes, washed with water, drummed, squeezed and stretched, vacuum dried, re-moisturized and softened to obtain waterproof leather;

[00...

Embodiment 3

[0037] Embodiment 3: the manufacture method of waterproof soft leather: comprise the following steps:

[0038] A: Waterproof treatment: ①. Squeeze the wet blue leather, shave it evenly, rewet, retan, and dye it; ②. Add 0.2% of the waterproof material baking soda and 0.2% of the weight of the leather to the leather treated in step ①. 1.5% polyacrylic acid derivative Jintan PA-11 is tuned in the drum pH When the value reaches 4, add Jintanquor SI, which accounts for 10% of the weight of the leather, and after turning for 75 minutes, add Zonyl602, which accounts for 3% of the weight of the leather, and then add 1.3% of formic acid to adjust pH When the value reaches 2.5, wash with water, change the bath, and adjust with formic acid pH When the value reaches 2.5, add metal salt chromium powder accounting for 3% of the leather weight, rotate for 75 minutes, wash with water, drum out, squeeze water and stretch, vacuum dry, regain moisture and vibrate softly to obtain waterproof lea...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

PUM

No PUM Login to View More

Abstract

The invention relates to a method for manufacturing waterproof soft-surface leather. The method comprises the steps of waterproofing treatment and finishing treatment, wherein the waterproofing treatment is as follows: adding a waterproof material (accounting for 0.1-0.3wt% of leather) and polyacrylic acid derivatives (accounting for 1-2wt% of the leather) into a big drum to regulate the pH value to 4-6, adding waterproof fat liquor (accounting for 8-12wt% of the leather), rotating for 50-90 minutes, adding fluorine waterproofing agent (accounting for 3-4wt% of the leather), adding 1.2-1.5% formic acid to regulate the pH value to 2.5-4.5, washing with water, changing bath, regulating the pH value to 2.5-4.5 by using formic acid, adding trivalent metal salt (accounting for 3wt% of the leather), rotating for 60-90 minutes, washing with water, discharging, squeezing to remove water, spreading, carrying out vacuum-drying, remoistening, and vibrating to soften the leather, thereby obtaining the waterproof leather. The leather manufactured by the method of the invention has the advantages of excellent dynamic waterproofing property, high-temperature yellowing resistance and light resistance, has physical and chemical indices and appearance properties of common vamp leather. The leather is the main material for shoemaking enterprises, especially for novel battle boots for People's Liberation Army and People's Armed Police.

Description

technical field [0001] The invention relates to a method for making leather, in particular to a method for making waterproof yellow cow soft leather. Background technique [0002] At present, the common cattle leather products are generally waterproofed for a short time by applying wax or water repellent on the surface, and the leather treated in this way is polished and painted on the surface. According to different test methods, leather waterproofing is divided into dynamic waterproofing and static waterproofing. Dynamic waterproofing only requires surface waterproofing, while dynamic waterproofing requires imitating the state of the upper during walking and testing the number of times the leather is bent in water, which requires high waterproofing. At present, most of the painted waterproof leathers on the market are only waterproof in the static state, and the waterproof performance is not high; the dynamic waterproof leather is limited to unpainted suede or split leath...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

Application Information

Patent Timeline
no application Login to View More
Patent Type & Authority Patents(China)
IPC IPC(8): C14C11/00C14C9/02C14C9/00
Inventor 朱自军
Owner JIHUA 3515 LEATHER & SHOES