Antibacterial negative potential component, as well as preparation method and application thereof
A composition and negative potential technology, applied in the field of water treatment, can solve the problems of the negative ion release ability, far-infrared ability, antibacterial and bacteriostatic ability are not ideal, and achieve the effect of inhibiting the growth of bacteria
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0039] The preparation method is as follows:
[0040] a. Prepare materials according to the following components and weight percentages:
[0041] Tourmaline 10%,
[0042] Amphibolite 5%,
[0043] Zeolite 15%,
[0044] Muyu Stone 20%,
[0045] Medical Stone 20%,
[0046] Serpentine 20%,
[0049] Silicon oxide 4%;
[0050] b. After the above-mentioned prepared raw materials are mixed, heat at 200°C for 6 hours, cool, pulverize and ball mill to 40 micron powder;
[0051] c. Adding deionized water to the pulverized and ball-milled powder, stirring, mixing evenly, and heat treatment (heating at 200° C. for 40 minutes) to prepare an antibacterial negative potential composition.
[0052] d, the antibacterial negative potential composition is further made into granules, and the steps are as follows: add deionized water and pottery clay powder in the antibacterial negative potential composition, stir, mix, granulate with a g...
Embodiment 2
[0054] The preparation method is as follows:
[0055] a. Prepare materials according to the following components and weight percentages:
[0056] Tourmaline 25%,
[0057] Amphibolite 10%,
[0058] Zeolite 5%,
[0059] Muyu Stone 5%,
[0060] Medical Stone 20%,
[0061] Serpentine 20%,
[0063] Zinc Oxide 5%,
[0064] Silicon oxide 5%;
[0065]b. After the above prepared raw materials are mixed, heat at 250°C for 5 hours, cool, pulverize and ball mill to 10 micron powder;
[0066] c. Adding deionized water to the pulverized and ball-milled powder, stirring, mixing uniformly, and heat treatment (heating at 300° C. for 20 minutes) to prepare an antibacterial negative potential composition.
[0067] d, the antibacterial negative potential composition is further made into granules, and the steps are as follows: add deionized water and pottery clay powder to the antibacterial negative potential composition, stir, mix, granulate with a granulator...
Embodiment 3
[0069] The preparation method is as follows:
[0070] a. Prepare materials according to the following components and weight percentages:
[0071] Tourmaline 20%,
[0072] Amphibolite 15%,
[0073] Zeolite 15%,
[0074] Muyu Stone 20%,
[0075] Medical Stone 15%,
[0076] Serpentine 5%,
[0077] Magnesium Oxide 4%,
[0078] Zinc Oxide 3%,
[0079] Silicon oxide 3%;
[0080] b. After the above-mentioned prepared raw materials are mixed, heat at 300°C for 4 hours, cool, pulverize and ball mill to 70 micron powder;
[0081] c. Add deionized water to the pulverized and ball-milled powder, stir, mix evenly, and heat treat (heat at 220° C. for 25 minutes) to prepare an antibacterial negative potential composition.
[0082] d, the antibacterial negative potential composition is further made into granules, and the steps are as follows: add deionized water and pottery clay powder in the antibacterial negative potential composition, stir, mix, granulate with a granulator, bake a...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com