Natural silk fiber and cotton fiber yarn interwoven fabric and production method thereof
A production method and technology of natural silk, applied in the production of interwoven fabrics of natural silk fibers and cotton fiber yarns, in the field of interwoven fabrics of natural silk fibers and cotton fiber yarns, can solve problems such as high prices and incompatible manufacturing processes, and achieve The price is right, the market popularization is improved, and the effect of reducing broken ends
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
specific Embodiment 1
[0035] Warp: 100s / 2 mercerized cotton yarn, weft: 22D / 3 cooked mulberry silk
[0036] (1) Yarn preparation: 100s / 2 mercerized cotton yarn is used as the warp yarn, and 22D / 3 cooked mulberry silk is used as the weft yarn;
[0037] (2) Preparation before weaving: 100s / 2 mercerized cotton yarn is used as the warp yarn, and cold sizing process is adopted: warping on the section warping machine, and cold sizing agent is used for sizing during the warping process to improve the weaving process of the yarn. Abrasion resistance and strength;
[0038] In the cold sizing process, the cold sizing agent is used for direct sizing: in the process of warping and reeling, the cold sizing liquid is directly placed on the warp yarn through the liquid supply roller of the sizing tank, and it is quickly dried at room temperature to form a film; the dosage is 3% of the sizing rate of the yarn ;
[0039] (3) Weaving: The rapier loom is used to weave the warp yarn of 100s / 2 mercerized cotton yarn ...
specific Embodiment 2
[0046] Warp: 22D / 6 cooked mulberry silk, weft: 80s / 2 mercerized cotton yarn
[0047] (1) Yarn preparation: 22D / 6 cooked mulberry silk is used as the warp yarn, and 80s / 2 mercerized cotton yarn is used as the weft yarn;
[0048] (2) Preparation before weaving: 22D / 6 cooked mulberry silk is used as the warp yarn, directly warped by a section warping machine, and the yarn is wound onto the weaving shaft according to the organization requirements of the fabric, without cold sizing;
[0049] (3) Weaving: A rapier loom is used to weave the warp yarn of 22D / 6 cooked mulberry silk and the weft yarn of 80s / 2 mercerized cotton yarn. ;
[0050] (4) Finishing: After weaving, the fabric is sequentially washed, dried, stretched, pre-shrunk, and polished to form an interwoven fabric of natural silk fiber and cotton fiber yarn.
[0051] The specific process parameters of each process in finishing are as follows:
[0052] Washing: open width washing method, washing temperature 60 ℃, PH valu...
specific Embodiment 3
[0056] Warp: 22D / 3 raw mulberry silk, weft: 100s / 2 mercerized cotton yarn
[0057] (1) Yarn preparation: 22D / 3 raw mulberry silk is used as the warp yarn, and 100s / 2 mercerized cotton yarn is used as the weft yarn;
[0058] (2) Preparation before weaving: 22D / 3 raw mulberry silk is used as the warp yarn, and the warping machine is directly used for warping, and the yarn is wound on the weaving shaft according to the organization requirements of the fabric, without cold sizing;
[0059] (3) Weaving: A rapier loom is used to weave the warp yarn of 22D / 3 raw mulberry silk and the weft yarn of 100s / 2 mercerized cotton yarn. The speed of the loom is 350 r / min, the upper machine tension is 1300N, and the heald leveling time is 310°;
[0060] (4) Finishing: After weaving, the fabric is refined, washed, dyed, washed, tenter-dried, pre-shrunk, and polished to form an interwoven fabric of natural silk fiber and cotton fiber yarn.
[0061] The specific process parameters of each process...