A production method and technology of artificial leather, applied in chemical instruments and methods, textiles and papermaking, heating/cooling fabrics, etc., can solve problems such as difficult to remove, screen ink pollution, increase the production cost of artificial leather, etc., and reduce the defective rate Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment
[0035] Embodiment: a kind of anti-screen ink pollution artificial leather manufacturing method, concrete steps are as follows:
[0036] Step 1: Mixing ingredients: 100 parts by weight of polyvinyl chloride resin, 30-50 parts by weight of plasticizer, 30-50 parts by weight of filler, 0.5-1 part by weight of lubricant, 2-5 parts by weight of heat-resistant stabilizer, 3 parts by weight of pigment ~5 parts by weight, 30~50 parts by weight of regulator and 1 part by weight of anti-screen ink pollution processing aid are mixed evenly in a high-speed dispersing mixer, the stirring temperature is 120°C-130°C, and the stirring time is 150s-250s;
[0037] Step 2: Mixing: discharge the homogeneously mixed materials in step 1 into the internal mixer for mixing, the mixing temperature is 130°C-150°C, and the mixing time is 200s-300s;
[0038] Step 3: Mastication: Discharge the mixed material to the rubber mixer, and carry out plastication at a temperature of 120°C to 130°C for 10min to 20...