A technology of synthetic leather and treatment agent, which is applied in fiber treatment, improved hand-feeling fibers, textiles and papermaking, etc. It can solve the problems of unsatisfactory aesthetics and hand feeling of consumers, achieve smooth hand feeling, increase cost, and unique contrast effect Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0026] At normal temperature and pressure, 20 parts by weight of modified polyurethane resin, 23 parts by weight of cyclohexanone, 12 parts by weight of xylene, 17 parts by weight of butyl acetate, 3 parts by weight of nano elastic powder, and 4 parts by weight of silicon matting powder, stir well at room temperature for at least 30 minutes, grind, filter, and discard the filter residue; add 2 parts by weight of amino silicone oil and 1 part by weight of castor oil to the resulting mixture, and stir evenly at room temperature; then add the remaining 18 parts by weight of the modified polyurethane resin was uniformly stirred at room temperature for at least 30 minutes until the viscosity was stable, and the finished product of the skin-feeling matte surface washing and brightening treatment agent for synthetic leather without precipitation and slightly yellowish transparent liquid was obtained.
[0027] See Table 1 for the performance index of the obtained synthetic leather matt...
Embodiment 2
[0032] At normal temperature and pressure, 15 parts by weight of modified polyurethane resin, 28 parts by weight of cyclohexanone, 10 parts by weight of xylene, 18 parts by weight of butyl acetate, 5 parts by weight of nano elastic powder, and 4 parts by weight of silicon matting powder, stirred thoroughly at room temperature for at least 30 minutes, ground, filtered, and discarded the filter residue; added 1.5 parts by weight of amino silicone oil and 0.5 parts by weight of castor oil to the resulting mixture, and stirred evenly at room temperature; then added the remaining 18 parts by weight of the modified polyurethane resin was uniformly stirred at room temperature for at least 30 minutes until the viscosity was stable, and the finished product of the skin-feeling matte surface washing and brightening treatment agent for synthetic leather without precipitation and slightly yellowish transparent liquid was obtained.
[0033] See Table 2 for the performance indexes of the obt...
Embodiment 3
[0038] At normal temperature and pressure, 20 parts by weight of modified polyurethane resin, 26 parts by weight of cyclohexanone, 11 parts by weight of xylene, 15 parts by weight of butyl acetate, 4 parts by weight of nano elastic powder, and 3 parts by weight of silicon matting powder, stir well at room temperature for at least 30 minutes, grind, filter, and discard the filter residue; add 2 parts by weight of amino silicone oil and 1 part by weight of castor oil to the resulting mixture, and stir evenly at room temperature; then add the remaining 18 parts by weight of the modified polyurethane resin was uniformly stirred at room temperature for at least 30 minutes until the viscosity was stable, and the finished product of the skin-feeling matte surface washing and brightening treatment agent for synthetic leather without precipitation and slightly yellowish transparent liquid was obtained.
[0039] See Table 3 for the performance index of the obtained skin-feeling matte sur...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com