A technology for generating negative ions and storing light, applied in the field of lampshades, can solve the problems of inability to use harmful pollutants, lack of light removal guidance and aesthetics, etc., to achieve the effects of improving immunity, promoting health, and improving living environment
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0017] The light-storing coating used in this embodiment, by mass percentage, is composed of: 65% zinc sulfide phosphor, 10% magnesium aluminum hydroxide, 10% cobalt aluminate, 5% magnesium oxide, and 2% calcium aluminate , CLEAR adhesive 8%. Mix all the components except the CLEAR binder evenly and pulverize into a uniform powder, then add the CLEAR binder, stir evenly, and apply it on the inner surface of the lampshade layer 1 with a coating thickness greater than 0.1mm, and let it dry naturally Finally, the light-storage paint relies on the function of the binder in its components to closely adhere to the inner wall of the lampshade layer 1 to form the light-storage paint layer 2 .
[0018] After the light-storing paint layer 2 is fully bonded and dried, the photocatalyst paint is coated on the light-storage paint layer 2, and the photocatalyst paint is composed of: nano-TiO 2 3%, ZnO5%, CdS2%, ZrO 2 1%, SnO 2 1%, WO 3 0.5%, 8% CLEAR binder, deionized water, and the res...
Embodiment 2
[0021] The light-storing coating used in this embodiment, by mass percentage, has the following components: 30% of zinc sulfide phosphor, 25% of magnesium aluminum hydroxide, 20% of cobalt aluminate, 10% of magnesium oxide, 7% of calcium aluminate, CLEAR adhesive 8% composition. Mix all the components except the CLEAR binder evenly and pulverize into a uniform powder, then add the CLEAR binder, stir evenly, and apply it on the inner surface of the lampshade layer 1 with a coating thickness greater than 0.1mm, and let it dry naturally Finally, the light-storage paint relies on the function of the binder in its components to closely adhere to the inner wall of the lampshade layer 1 to form the light-storage paint layer 2 .
[0022] After the light-storing paint layer 2 is fully bonded and dried, the photocatalyst paint is coated on the light-storage paint layer 2, and the photocatalyst paint is composed of: nano-TiO 2 1%, ZnO2%, CdS4%, ZrO 2 2%, SnO 2 2%, WO 3 1.5%, 6% CLEAR...