Paper preparing process
A preparation process and paper technology, applied in the field of paper preparation process, can solve problems such as excessive use, residue, and reduced utilization rate of paper-making chemicals, and achieve the effects of reducing residue, reducing usage, and improving use efficiency
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
preparation example Construction
[0010] The preparation technology of paper of the present invention, it comprises the steps:
[0011] (1) Provide softwood pulp and hardwood pulp, wherein the dry mass ratio of hardwood pulp to softwood pulp is between 1 and 4, and deflake the softwood pulp and hardwood pulp respectively.
[0012] The deflaking step uses a deflaking machine. During deflaking, it is preferable to control the mass percentage concentration of softwood pulp and hardwood pulp to be 3% to 15%, respectively. The effect of deflaking in this concentration range is better.
[0013] In the process of defibering, besides shearing, kneading and carding, the cell wall of the fiber also undergoes displacement, deformation and rupture to absorb water and swell, resulting in fine fibrilization, which makes the pulp soft and plastic, and also makes the fiber More hydroxyl groups are exposed in the protein molecular chain, which improves the binding force between fibers.
[0014] The fluffed softwood pulp and h...
Embodiment 1
[0025] The softener from Buckman Company is used, and the amount of softener is 0.286% of the dry mass of hardwood fiber. The mass ratio of hardwood pulp to softwood pulp is 70:30. The mass percent concentration of fiber is 5% during the process, and then the hardwood pulp is refined for 1000 rpm, and the softwood pulp is refined for 2500 rpm. Put it into hardwood pulp for 5 minutes, then add coniferous pulp to mix with it, and make sheets after mixing, the basis weight of the paper is 30g / m 2 .
[0026] After testing, the paper made by this method has a breaking length of 2.06km.
Embodiment 2
[0032] The softener from Buckman Company is used, and the amount of softener is 1.429% of the dry mass of hardwood fiber. The mass ratio of hardwood pulp to softwood pulp is 70:30. The mass percent concentration of fiber is 5% during the process, and then the hardwood pulp is refined for 1000 rpm, and the softwood pulp is refined for 2500 rpm. Put it into hardwood pulp for 5 minutes, then add coniferous pulp to mix with it, and make sheets after mixing, the basis weight of the paper is 30g / m 2 .
[0033] After testing, the paper made by this method has a breaking length of 1.10km.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com