Comfortable high-emulation wool fabric, production technology thereof and textile thereof
A production process and fiber technology, applied in the field of production workers, comfortable and high-quality wool-like fiber fabrics, can solve the problems of poor wool-like fabric softness, material selection and processing technology need to be improved, easy to fluff, etc., so as to reduce fluff and lint. Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0020] A kind of production technology of comfortable high wool-like fiber fabric, comprises the following steps:
[0021] (1) In the warp direction, the blended yarn composed of polyester fiber, bamboo charcoal fiber, fine denier viscose fiber and spandex fiber is 20%: 30%: 35%: 15% according to the dry weight ratio as the warp yarn, and the warp yarn specification is 25.2 tex; in the weft direction, the blended yarn composed of cotton fiber, tencel, vegetable protein fiber and conductive fiber is 30%: 10%: 35%: 25% according to the dry weight ratio as the weft yarn, and the specification of the warp yarn is 27.6tex;
[0022] (2) The dyeing step is to pre-treat wool with reactive dyes at 60°C for 20 minutes, then cool to room temperature, and then heat up twice. The first time the temperature is raised from room temperature to 52°C, the heating rate is controlled within one minute. Raise the temperature by one degree; after reaching this stage, keep warm for 15 minutes, then ...
Embodiment 2
[0028] A kind of production technology of comfortable high wool-like fiber fabric, comprises the following steps:
[0029] (1) In the warp direction, the blended yarn composed of polyester fiber, bamboo charcoal fiber, fine denier viscose fiber and spandex fiber is 20%: 30%: 35%: 15% according to the dry weight ratio as the warp yarn, and the warp yarn specification is 25.2 tex; in the weft direction, the blended yarn composed of cotton fiber, tencel, vegetable protein fiber and conductive fiber is 30%: 10%: 35%: 25% according to the dry weight ratio as the weft yarn, and the specification of the warp yarn is 27.6tex;
[0030] (2) The dyeing step is to pre-treat wool with reactive dyes at 60°C for 20 minutes, then cool to room temperature, and then heat up twice. The first time the temperature is raised from room temperature to 50°C, the heating rate is controlled within one minute. Raise the temperature by one degree; after reaching this stage, keep warm for 15 minutes, then ...
Embodiment 3
[0036] A kind of production technology of comfortable high wool-like fiber fabric, comprises the following steps:
[0037] (1) In the warp direction, the blended yarn composed of polyester fiber, bamboo charcoal fiber, fine denier viscose fiber and spandex fiber is 20%: 30%: 35%: 15% according to the dry weight ratio as the warp yarn, and the warp yarn specification is 25.2 tex; in the weft direction, the blended yarn composed of cotton fiber, tencel, vegetable protein fiber and conductive fiber is 30%: 10%: 35%: 25% according to the dry weight ratio as the weft yarn, and the specification of the warp yarn is 27.6tex;
[0038] (2) The dyeing step is to pre-treat wool with reactive dyes at 60°C for 20 minutes, then cool to room temperature, and then heat up twice. The first time the temperature is raised from room temperature to 54°C, the heating rate is controlled within one minute. Raise the temperature by one degree; after reaching this stage, keep warm for 15 minutes, then ...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com