Bentonite/modified zeolite compound super absorbent cat litter
A technology of modified zeolite and high water absorption, applied in animal houses, applications, animal husbandry, etc., can solve the problem of water absorption performance to be improved, and achieve the effect of improving deodorization function, improving water absorption, and not polluting the environment
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment Construction
[0024] A kind of bentonite / modified zeolite composite superabsorbent cat litter, the weight percent of its raw material component is:
[0025] Sodium bentonite 55%
[0026] Modified Zeolite 20%
[0027] Carboxymethylcellulose 6%
[0028] Nano carbon 3%
[0029] Bran 12%
[0030] Polyacrylamide 4%.
[0031] The preparation method of the modified zeolite is as follows: roast the zeolite at 400°C for 4 hours, crush it, and pass through a 60-mesh sieve; after sieving, put the zeolite into 1mol / L hydrochloric acid and soak it for 10 hours, wash it, dry it, and put it into Soak in 1mol / L sodium chloride solution for 10 hours, wash and dry.
[0032] Mix sodium-based bentonite, modified zeolite, nano-carbon, and bran evenly, pulverize, grind and pass through a 150-mesh sieve; then mix the sieved powder evenly with polyacrylamide and carboxymethyl cellulose, and wet granulate , particle size is 3mm, drying is the finished product.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com