An environmentally friendly water and automobile technology, applied in the direction of polyurea/polyurethane coatings, coatings, etc., can solve the problems of affecting color, weak metal texture, insufficient silver powder arrangement, etc., to reduce pollution, good arrangement effect, and reduce VOC. The effect of emissions
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0027] A preparation method of environment-friendly water-clear automotive original paint, the method comprises the following process steps:
[0028] (1) First add 35kg of water-based resin (Bayhydrol XP2648), 1.6kg of co-solvent propylene glycol monomethyl ether and 33.4kg of deionized water in a stirring state and mix them uniformly to obtain mixture a, which is the same as adjusting mixture a by pH regulator NaOH The pH value is 7.5-8.5;
[0029] (2) Add water-based amino resin cymel3283kg, water-based thickener Viscalex HV303kg, and deionized water 12kg into the above-mentioned mixture a in sequence, and stir evenly to obtain mixture b;
[0030] (3) Water-based resin (Bayhydrol XP2648) 6kg, water-based dispersant TEGO Dispers715W) 7.5kg, cosolvent diol monomethyl ether 42kg deionized water 2.5kg, metal pigment STAPA HYDROLAN219240kg are mixed in turn, and stir to obtain mixture c; then Add 12% of the weight of the mixture c into the mixture b obtained in step (2), and sti...
Embodiment 2
[0032] A preparation method of environment-friendly water-clear automotive original paint, the method comprises the following process steps:
[0033] (1) First add 30kg of water-based resin (Bayhydrol XP2621), 1.6kg of co-solvent propylene glycol monomethyl ether and 38.4kg of deionized water in a stirring state and mix them uniformly to obtain mixture a, which is the same as adjusting mixture a by pH regulator KOH The pH value is 7.5-8.5;
[0034] (2) Add water-based amino resin cymel3283kg water-based thickener Rheolate6783kg, deionized water 12.kg into the above mixture a in turn, and stir evenly to obtain mixture b;
[0035] (3) Water-based resin (Bayhydrol XP2621) 6kg, water-based dispersant TEGO Dispers745W) 7.5kg, cosolvent diol monomethyl ether 42kg deionized water 2.5kg, metal pigment STAPA HYDROLAN215340kg are mixed successively, and stir to obtain mixture c; Add it into the mixture b obtained in step (2) at a ratio of 11% of the weight of the mixture c, and stir ev...
Embodiment 3
[0037] A preparation method of environment-friendly water-clear automotive original paint, the method comprises the following process steps:
[0038] (1) First add 32kg of water-based resin (Bayhydrol XP2621), 1.6kg of co-solvent propylene glycol monomethyl ether and 36.4kg of deionized water in a stirring state and mix them uniformly to obtain mixture a, which is the same as adjusting mixture a by pH regulator NaOH The pH value is 7.5-8.5;
[0039] (2) Add water-based amino resin cymel3283kg water-based thickener Viscalex HV303kg, deionized water 12kg into the above mixture a in turn, and stir evenly to obtain mixture b;
[0040] (3) 6kg of water-based resin (Bayhydrol XP2621), 7.5kg of water-based dispersant (TEGO Dispers740W), 2.5kg of cosolvent glycol monomethyl ether 42kg of deionized water, and metal pigment STAPA HYDROLAN215640kg were mixed in sequence, and stirred evenly to obtain mixture c; then Add 12% of the weight of the mixture c into the mixture b obtained in st...
PUM

Abstract
Description
Claims
Application Information

- R&D
- Intellectual Property
- Life Sciences
- Materials
- Tech Scout
- Unparalleled Data Quality
- Higher Quality Content
- 60% Fewer Hallucinations
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2025 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com