[0026] Embodiment: a kind of double-sided leather manufacturing method, concrete steps are as follows:
[0027] Step 1: Wet Mixing Ingredients:
[0028] a. Stir 5~10kg of dimethylformamide and 0.5~2kg of color paste at high speed for 80~100 minutes, then filter for use;
[0029] b. 100~120kg of dimethylformamide and 20~30kg of wood flour are mixed and stirred for 20~30 minutes, then fully swollen for 30~40 minutes, and then the mixture filtered in step a is added and stirred evenly for use;
[0030] c. Add 100kg of wet polyurethane resin to the mixture formed in step b, stir for 30-40 minutes, and degas for 40-50 minutes;
[0031] Step 2: Wet Bass Production:
[0032] Smear and scrape the slurry formed by defoaming in step 1 on the smooth surface of the warp-knitted suede (the other side of the suede is the rough surface), and then immerse it in dimethyl methacrylate with a concentration of 18-22% by mass. coagulate in an aqueous solution of methylformamide, then go through...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com