Making technology for handbag
A production process and handbag technology, applied in the field of handbags, can solve the problems of affecting the normal use of handbags, difficult to guarantee the yield rate, and high cost of raw materials, and achieve the effects of eliminating the tedious maintenance, easy operation, and simple production process.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
specific Embodiment 1
[0039] Use soft PVC as the main raw material.
[0040] First, the raw materials are configured according to the ratio of soft PVC weight ratio of 99.92% and colorant weight ratio of 0.08%, and the aforementioned raw materials are placed in a mixer, and stirred at normal temperature and pressure for 2 to 8 minutes to stir evenly;
[0041] Secondly, inject the uniformly stirred raw materials into the first mold, the second mold and the third mold respectively, and heat each molding mold at 140°C-230°C under normal pressure, and the heating time must be less than 5 minutes. to form the body, bottom, handles and / or shoulder straps of handbags;
[0042] Next, under normal pressure, cooperate with the oil temperature machine to cool the injection molded molds for 30 to 150 seconds, and open the mold to take out the main body, bottom, handle and / or shoulder strap of the handbag;
[0043] Finally, sew the removed main body and the bottom of the bag at the joint through the thread bod...
specific Embodiment 2
[0044] Use soft PVC as the main raw material.
[0045] First, configure the raw materials in a ratio of 99.96% by weight of soft PVC and 0.04% by weight of the coloring agent. The raw materials are placed in a mixer and stirred at room temperature and pressure for 2 to 8 minutes to stir evenly;
[0046] Secondly, inject the uniformly stirred raw materials into the first mold, the second mold and the third mold respectively, and heat each molding mold at 140°C-230°C under normal pressure, and the heating time must be less than 5 minutes. to form the body, bottom, handles and / or shoulder straps of handbags;
[0047] Next, under normal pressure, cooperate with the cooling tower to cool the injection molded molds for 30 to 150 seconds, and open the mold to take out the main body, bottom, handle and / or shoulder strap of the handbag;
[0048]Finally, sew the removed main body and the bottom of the bag at the joint through the thread body to make the bag body of the handbag. The re...
specific Embodiment 3
[0049] Use soft PVC as the main raw material.
[0050] First, configure the raw materials in a ratio of 99.97% by weight of soft PVC and 0.03% by weight of the coloring agent. At the same time, mix the flavoring agent into the raw material. The raw materials are placed in a mixer and stirred at room temperature and pressure for 2 to 8 minutes to stir evenly;
[0051] Secondly, inject the uniformly stirred raw materials into the first mold, the second mold and the third mold respectively, and heat each molding mold at 140°C-230°C under normal pressure, and the heating time must be less than 5 minutes. to form the body, bottom, handles and / or shoulder straps of handbags;
[0052] Next, under normal pressure, cooperate with a chiller to cool each molding mold that has completed injection molding for 30 to 150 seconds, and open the mold to take out the main body, bottom, handle and / or shoulder strap of the handbag;
[0053] Finally, sew the removed main body and the bottom of th...