Preparation method for elastic fabric
A fabric and elastic technology, which is applied in the field of elastic fabric preparation, can solve the problems of inability to effectively ensure the elasticity of polyester-spandex elastic fabric, Zou effect, feel and comfort, and poor flame retardancy of fabrics, and achieve light and soft hand feeling, color Fast coloring and strong flame retardancy
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0018] Embodiment 1: the preparation method of described elastic fabric, described weaving process comprises successively:
[0019] S1: Warping;
[0020] S2: sizing: this process step adopts the mixed slurry sizing of deformed starch and PVA, controls the temperature of mixed slurry 40 ℃~45 ℃;
[0021] S3: parallel axis;
[0022] S4: Gray fabric weaving, this process step adopts air jet weaving, choose high tension on the machine, high back beam, early shedding and early weft spraying;
[0023] S5: Dyeing, this process step adopts the dyeing method of staged heating and staged cooling, specifically: first, keep warm at 60°C-65°C for 20-25min, then rise to 96°C-97°C and keep warm for 30-40min, and then cool down To 60 ℃ ~ 65 ℃, keep warm for 20 ~ 25 minutes, then lower to room temperature, drain and wash with water, and finally dry at 170 ℃;
[0024] S6: Impregnation flame retardant treatment, specifically put the fabric into a vacuum pressurized tank to evacuate to make the...
Embodiment 2
[0027] Embodiment 2: the preparation method of described elastic fabric, described weaving process comprises successively:
[0028] S1: Warping;
[0029] S2: sizing: this process step adopts the mixed slurry sizing of deformed starch and PVA, controls the temperature of mixed slurry 40 ℃~45 ℃;
[0030] S3: parallel axis;
[0031] S4: Gray fabric weaving, this process step adopts air jet weaving, choose high tension on the machine, high back beam, early shedding and early weft spraying;
[0032] S5: Dyeing, this process step adopts the dyeing method of staged heating and staged cooling, specifically: first, keep warm at 60°C-65°C for 20-25min, then rise to 96°C-97°C and keep warm for 30-40min, and then cool down To 60 ℃ ~ 65 ℃, keep warm for 20 ~ 25 minutes, then lower to room temperature, drain and wash with water, and finally dry at 170 ℃;
[0033] S6: Impregnation flame retardant treatment, specifically put the fabric into a vacuum pressurized tank to evacuate to make the...
Embodiment 3
[0036] Embodiment 3: the preparation method of described elastic fabric, described weaving process comprises successively:
[0037] S1: Warping;
[0038] S2: sizing: this process step adopts the mixed slurry sizing of deformed starch and PVA, controls the temperature of mixed slurry 40 ℃~45 ℃;
[0039] S3: parallel axis;
[0040] S4: Gray fabric weaving, this process step adopts air jet weaving, choose high tension on the machine, high back beam, early shedding and early weft spraying;
[0041] S5: Dyeing, this process step adopts the dyeing method of staged heating and staged cooling, specifically: first, keep warm at 60°C-65°C for 20-25min, then rise to 96°C-97°C and keep warm for 30-40min, and then cool down To 60 ℃ ~ 65 ℃, keep warm for 20 ~ 25 minutes, then lower to room temperature, drain and wash with water, and finally dry at 170 ℃;
[0042] S6: Impregnation flame retardant treatment, specifically put the fabric into a vacuum pressurized tank to evacuate to make the...
PUM
Login to View More Abstract
Description
Claims
Application Information
Login to View More