Tailor's chalk
A technology based on weight percentage and calcium sulfate, which is applied in dyeing, textiles and papermaking, etc., can solve the problems of human body injury, easy to be gasified, easy to cause lung diseases, etc., and achieve the effect of easy removal
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
preparation example Construction
[0016] The preparation method of this chalk powder comprises the following steps:
[0017] 1. By weight percentage, calcium sulfate 60%-65%, salicylic acid 15%-17%, calcium oxide 15%-16%, zinc stearate 3.2%-5.0%, calcium stearate 2%-5% %, palmitic acid 0% ~ 10%, amino acid 0% ~ 1%, release agent 0.2% ~ 0.3%, heating and stirring at a constant temperature of 80 ~ 90 degrees to dissolve completely, forming a uniform colorless transparent solution or milky white solution , stop heating, and keep the solution warm at 20-25 degrees;
[0018] 2. Soak the prepared chalk in the above solution, take it out after 15-50 minutes, and let it dry naturally to prepare the chalk.
[0019] The scribing powder of the present invention is improved on the basis of the existing invisible scribing powder. Combining with the traditional scribing powder, the main component of the developed scribing powder is calcium sulfate. Since calcium sulfate is equipped with other auxiliary materials, it is ve...
Embodiment 1
[0021] The calcined powder comprises 60% of calcium sulfate, 15% to 17% of salicylic acid, 15% to 16% of calcium oxide, 3.2% to 5.0% of zinc stearate, 2% to 5% of calcium stearate, palm Acid 0% to 10%, amino acid 0% to 1%, release agent 0.2% to 0.3%, and the rest are impurities.
[0022] Calcium sulfate, salicylic acid, calcium oxide, zinc stearate, calcium stearate, palmitic acid, amino acid, and release agent are heated and stirred at a constant temperature of 80 to 90 degrees to completely dissolve them in percent by weight, and Uniform colorless and transparent solution or milky white solution, stop heating, keep the solution warm at 20-25 degrees; soak the prepared marking powder in the above solution, take it out after 15-50 minutes, and dry it naturally to complete the marking pink.
Embodiment 2
[0024] The calcined powder comprises 65% of calcium sulfate, 15% to 17% of salicylic acid, 15% to 16% of calcium oxide, 3.2% to 5.0% of zinc stearate, 2% to 5% of calcium stearate, palm Acid 0% to 10%, amino acid 0% to 1%, release agent 0.2% to 0.3%, and the rest are impurities.
[0025] Calcium sulfate, salicylic acid, calcium oxide, zinc stearate, calcium stearate, palmitic acid, amino acid, and release agent are heated and stirred at a constant temperature of 80 to 90 degrees to completely dissolve them in percent by weight, and Uniform colorless and transparent solution or milky white solution, stop heating, keep the solution warm at 20-25 degrees; soak the prepared marking powder in the above solution, take it out after 15-50 minutes, and dry it naturally to complete the marking pink.
PUM
Login to View More Abstract
Description
Claims
Application Information
Login to View More