Method for improving cooling performance of cooling oil
A technology of cooling performance and cooling oil, applied in chemical instruments and methods, petroleum industry, materials for heat exchange, etc., can solve the problem of poor thermal conductivity of cooling oil, etc., and achieve the effect of improving cooling performance
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0008] Embodiment 1, the method for improving the cooling performance of cooling oil in this embodiment is to add submicron copper powder to the base cooling oil, and the mass ratio of the submicron copper powder to the base cooling oil is 2:100, of course, in specific implementation The mass ratio of the submicron copper powder to the base cooling oil can also be other values within the range of 1-10:100, and the diameter of the submicron copper powder is 0.1-5.0 microns.
Embodiment 2
[0009] Embodiment 2, the method for improving the cooling performance of cooling oil in this embodiment is to add submicron copper powder to the base cooling oil, the mass ratio of the submicron copper powder to the base cooling oil is 6:100, and the submicron copper powder The diameter of the powder is 0.1-5.0 microns.
Embodiment 3
[0010] Embodiment 3, the method for improving the cooling performance of cooling oil in this embodiment is to add submicron copper powder to the base cooling oil, the mass ratio of the submicron copper powder to the base cooling oil is 8:100, and the submicron copper powder The diameter of the powder is 0.1-5.0 microns.
[0011] The cooling oil in the above-mentioned embodiments one to three can be prepared by the following method:
[0012] (1) Add sub-micron copper powder and deionized water to form a slurry with a concentration of 110-150g / L. After standing for 90-120 seconds, take the above slurry and separate and remove it by suspension separation and filtration and sieving. The large copper powder particles in the submicron copper powder make the particle size and diameter between 1.5 and 4.5 microns;
[0013] (2), adopt vacuum filtration method, repeatedly wash and separate the soluble salt in the slurry with deionized water, check until there is no sulfate ion with the...
PUM
Property | Measurement | Unit |
---|---|---|
diameter | aaaaa | aaaaa |
thermal conductivity | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com