Embodiment 1
[0024] A process for simultaneously dyeing nylon and spandex, the steps are as follows:
[0025] (1) Pre-dyeing: put the product into the dyeing vat, control the pH value to 4.7, and the temperature at 30°C, add 2g / L spandex colorant to the dye bath, and heat up at a rate of 2°C until the dye bath temperature reaches 50°C. Cycle for 20 minutes;
[0026] (2) Dyeing: Cool down at a rate of 2°C until the temperature of the dyeing bath reaches 30°C, add 0.1g / L dye to the dye vat to dye spandex, then add 1.5g / L nylon dye, control the temperature to 30°C, cycle 5 minute;
[0027] (3) Auxiliary dyeing: Add auxiliary agents to the dyeing vat, control the temperature at 30°C, circulate for 5 minutes, then raise the temperature at a rate of 2°C per minute until the temperature of the dyeing bath reaches 100°C, and keep warm for 30 minutes;
[0028] (4) Check the sample until the color is accurate, wash it out of the tank, dry it, and fix the color.
Embodiment 2
[0030] A process for simultaneously dyeing nylon and spandex, the steps are as follows:
[0031] (1) Pre-dyeing: put the product into the dyeing vat, control the pH value to 4.7, and the temperature at 30°C, add 3g / L spandex colorant to the dye bath, and heat up at a rate of 2°C until the dye bath temperature reaches 50°C. Cycle for 20 minutes;
[0032] (2) Dyeing: Cool down at a rate of 2°C until the temperature of the dyeing bath reaches 30°C, add 0.15g / L dye to the dye vat to dye spandex, then add 1.5g / L nylon dye, control the temperature to 30°C, cycle 5 minute;
[0033] (3) Auxiliary dyeing: Add auxiliary agents to the dyeing vat, control the temperature at 30°C, circulate for 5 minutes, then raise the temperature at a rate of 2°C per minute until the temperature of the dyeing bath reaches 100°C, and keep warm for 30 minutes;
[0034] (4) Check the sample until the color is accurate, wash it out of the tank, dry it, and fix the color.
Embodiment 3
[0036] A process for simultaneously dyeing nylon and spandex, the steps are as follows:
[0037] (1) Pre-dyeing: put the product into the dyeing vat, control the pH value to 4.7, and the temperature at 30°C, add 4g / L spandex colorant to the dye bath, and heat up at a rate of 2°C until the dye bath temperature reaches 50°C. Cycle for 20 minutes;
[0038] (2) Dyeing: Cool down at a rate of 2°C until the temperature of the dyeing bath reaches 30°C, add 0.2g / L dye to the dye vat to dye spandex, then add 1.5g / L nylon dye, control the temperature to 30°C, cycle 5 minute;
[0039] (3) Auxiliary dyeing: Add auxiliary agents to the dyeing vat, control the temperature at 30°C, circulate for 5 minutes, then raise the temperature at a rate of 2°C per minute until the temperature of the dyeing bath reaches 100°C, and keep warm for 30 minutes;
[0040] (4) Check the sample until the color is accurate, wash it out of the tank, dry it, and fix the color.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology