Anti-crease and anti-shrink finishing process for wool fabric
An anti-shrinkage finishing and fabric technology, applied in the field of wool anti-wrinkle and anti-felting shrinkage, can solve problems such as strong wool damage, and achieve the effects of improving anti-wrinkle performance, increasing wet friction coefficient, and improving anti-felting resistance.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0036] A process for the anti-wrinkle and anti-shrink finishing of wool fabrics, including anti-wrinkle and anti-shrink finishing, washing and natural drying. The anti-wrinkle and anti-shrink finishing includes: firstly subjecting the wool fabric to plasma pretreatment, and then using transglutaminase to treat the plasma In the transglutaminase treatment, the concentration of transglutaminase is 13% (owf), the treatment temperature is 30°C, the treatment time is 30 minutes, and the treatment bath ratio is 1: 15; Afterwards, use a specific durable anti-wrinkle and shrink-proof finishing agent to perform anti-wrinkle finishing on the wool fabric using a two-soak and two-roll finishing process; the parameters of the two-soak and two-roll finishing process are: the nip rate is 75-80%; 80 Pre-baking at ℃ for 3 min; baking at 120 ℃ for 5 min; the durable anti-wrinkle and shrink-proof finishing agent is composed of the following components: in parts by weight,
[0037] Dimethylolurea re...
Embodiment 2
[0050] A process for the anti-wrinkle and anti-shrink finishing of wool fabrics, including anti-wrinkle and anti-shrink finishing, washing and natural drying. The anti-wrinkle and anti-shrink finishing includes: firstly subjecting the wool fabric to plasma pretreatment, and then using transglutaminase to treat the plasma In the transglutaminase treatment, the transglutaminase concentration is 25% (owf), the treatment temperature is 45°C, the treatment time is 30 minutes, and the treatment bath ratio is 1: 20; Afterwards, use a specific durable anti-wrinkle and shrink-proof finishing agent to perform anti-wrinkle finishing on the wool fabric using a two-soak and two-roll finishing process; the parameters of the two-soak and two-roll finishing process are: the nip rate is 75-80%; 90 Pre-baking at ℃ for 1 min; baking at 180 ℃ for 2 min; the durable anti-wrinkle and anti-shrink finishing agent consists of the following components: in parts by weight,
[0051] Dimethylolurea resin 18 ...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com