Machining method for constant-arc contact special-shaped bank
A processing method and special-shaped row technology, which is applied in the field of processing fixed-arc contact special-shaped rows, can solve the problems of rough surface, low surface hardness, and large accumulated errors, so as to reduce surface roughness, increase surface hardness, and reduce processing errors Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment Construction
[0009] The following structural drawings further describe the present invention:
[0010] A processing method for a special-shaped row of fixed-arc contacts, comprising the following steps: smelting - mold hot extrusion semi-forming - mold cold extrusion forming and surface hardening - cutting material - milling both sides - milling 3 slots. The smelting process described is as follows: the smelting furnace is heated up to 1100°C, and electrolytic copper and charcoal are put in for deoxidation, and 0.3 ~ 1.2% sterling silver, add 0.05 after another hour ~ 0.5% rare earth, the furnace temperature rises to 1125 ℃ for 2 hours before pouring copper rods. In actual implementation, due to the specific shape of the product, it is difficult to extrude and form, so the design adopts the shape of the product to move up the center of the mold, so that the positive extrusion force of the extruder mainly acts on the side with a large amount of deformation; an auxiliary oil cylinder is add...
PUM
Login to View More Abstract
Description
Claims
Application Information
Login to View More 