Metal cleaner material composition and preparation method and application of metal cleaner
A technology of metal cleaning agent and material composition, which is applied in the field of production and preparation of metal cleaning materials, can solve the problems of easy corrosion of metal, difficult to clean, clean up, etc., and achieve the effect of reducing maintenance costs, improving use efficiency and production efficiency
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
preparation example Construction
[0018] The present invention also provides a method for preparing a metal cleaning agent, wherein the preparation method comprises: mixing water, sodium sulfate, sodium chloride, calcium chloride, polyvinyl alcohol, phosphoric acid, starch, titanium dioxide and calcium carbonate Prepare metal cleaning agent; Wherein,
[0019] Relative to 100 parts by weight of the water, the amount of sodium sulfate is 5-15 parts by weight, the amount of sodium chloride is 3-10 parts by weight, and the amount of calcium chloride is 3-10 parts by weight , the consumption of the polyvinyl alcohol is 5-15 parts by weight, the consumption of the phosphoric acid is 20-50 parts by weight, the consumption of the starch is 1-10 parts by weight, and the consumption of the titanium dioxide is 3-15 parts by weight , the consumption of described calcium carbonate is 5-20 weight part.
[0020] Likewise, in a preferred embodiment of the present invention, relative to 100 parts by weight of the water, the a...
Embodiment 1
[0027] Mix 100g of water, 8g of sodium sulfate, 5g of sodium chloride, 5g of calcium chloride, 8g of polyvinyl alcohol, 30g of phosphoric acid, 3g of starch, 5g of titanium dioxide and 10g of calcium carbonate, and place it at a temperature of 40°C with a stirring rate of 100r / min Under the condition of stirring for 10min, the metal cleaning agent A1 was prepared.
Embodiment 2
[0029] Mix 100g of water, 12g of sodium sulfate, 8g of sodium chloride, 8g of calcium chloride, 12g of polyvinyl alcohol, 40g of phosphoric acid, 7g of starch, 10g of titanium dioxide and 15g of calcium carbonate and place it at a temperature of 80°C with a stirring speed of 200r / min Under the condition of stirring for 30min, the metal cleaning agent A2 was prepared.
PUM
| Property | Measurement | Unit |
|---|---|---|
| Particle size | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
Login to View More - R&D
- Intellectual Property
- Life Sciences
- Materials
- Tech Scout
- Unparalleled Data Quality
- Higher Quality Content
- 60% Fewer Hallucinations
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2025 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com