Unlock instant, AI-driven research and patent intelligence for your innovation.

A process for coking coal raw materials containing low-rank coal

A low-rank coal and raw material technology, which is applied in the field of coking technology, can solve the problems of low utilization of tamping coke ovens, overcapacity, and low-rank coal that cannot be applied on a large scale. It is of great significance for development and utilization, and it is easy to push coke , the effect of not easy pulverization

Active Publication Date: 2019-01-11
BEIJING SJ ENVIRONMENTAL PROTECTION & NEW MATERIAL CO LTD
View PDF5 Cites 0 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

[0006] In order to solve the problem that low-rank coal cannot be applied on a large scale in the prior art and the problems of overcapacity in the existing coking industry and low utilization of tamping coke ovens, a method for coking coal raw materials containing low-rank coal is provided. craft

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0030] (1) Pulverize sub-bituminous coal and mix it with additives to form low-rank coal raw material, and then mix it with pulverized 1 / 3 coking coal to form raw coal, and use tamping equipment to tamp the raw coal, wherein, by mass, The addition amount of auxiliary agent is 40wt% of the mass of sub-bituminous coal, the addition amount of said sub-bituminous coal is 65wt% of the mass of said raw coal, the G value of said sub-bituminous coal is 45, and the volatile matter content is 65%. The agent is asphaltene with a softening point of 105°C, and the asphaltene loses 45% in dry distillation in the absence of air at 850°C;

[0031] (2) Push the formed raw coal into the coke oven for coking, control the coking temperature to 850°C, and coking time for 16 hours, collect the overflowing mixture of crude gas, tar and crude benzene, and obtain coke as a by-product;

[0032] Adopt conventional process to separate crude gas and tar, and further separate crude benzene from tar, the am...

Embodiment 2

[0034] (1) Pulverize sub-bituminous coal and mix it with additives to form low-rank coal raw materials, and then form raw coal with pulverized 1 / 3 coking coal, and use tamping equipment to tamp and shape the raw coal, wherein, in terms of mass, auxiliary The added quality of the additive is 35wt% of the mass of the sub-bituminous coal, the added amount of the sub-bituminous coal is 50wt% of the mass of the raw coal, the G value of the sub-bituminous coal is 40, and the volatile content is 70%. It is an asphaltene with a softening point of 115°C, and the asphaltene loses 40% in dry distillation in the absence of air at 850°C;

[0035] (2) Push the formed raw coal into the coke oven for coking, control the coking temperature to 900°C, and coking time for 15.5 hours, collect the overflowing mixture of crude gas, tar and crude benzene, and obtain coke as a by-product;

[0036] Adopt conventional process to separate crude gas, tar, and further separate crude benzene from tar, the a...

Embodiment 3

[0038] (1) Pulverize sub-bituminous coal and mix it with additives to form low-rank coal raw material, and then mix it with pulverized 1 / 3 coking coal to form raw coal, and use tamping equipment to tamp the raw coal, wherein, by mass, The added quality of auxiliary agent is 30wt% of the mass of sub-bituminous coal, the added amount of said sub-bituminous coal is 70wt% of the mass of said raw coal, the G value of said sub-bituminous coal is 35, and the volatile matter content is 45%. The agent is asphaltene with a softening point of 120°C, and the asphaltene loses 42% in dry distillation in the absence of air at 850°C;

[0039] (2) Push the formed raw coal into the coke oven for coking, control the coking temperature to 950°C, and coking time for 17 hours, collect the overflowing mixture of crude gas, tar and crude benzene, and obtain coke as a by-product;

[0040] Adopt conventional process to separate crude gas, tar, and further separate crude benzene from tar, the amount of ...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

PUM

PropertyMeasurementUnit
softening pointaaaaaaaaaa
softening pointaaaaaaaaaa
softening pointaaaaaaaaaa
Login to View More

Abstract

The present invention discloses a process for coking a coal raw material containing low-rank coal. The process comprises: (1) crushing low-rank coal, mixing the crushed low-rank coal and an auxiliary agent to form a low-rank coal raw material, mixing the obtained low-rank coal raw material and a crushed middle-rank coal raw material or crushed high-rank coal material or crushed medium-high-rank coal raw material to form raw material coal, and carrying out stamp-charging molding on the raw material coal by using stamp-charging equipment; and (2) pushing the molded raw material coal into a coke oven, coking, and collecting the overflowed crude coal gas, tar and crude benzene mixture while obtaining the byproduct coke, wherein the coking temperature is controlled at more than 800 DEG C, the coking time is not less than 15 h, and the auxiliary agent is an organic binder with air isolated dry distillation weightlessness of less than 50% at a temperature of 850 DEG C. According to the present invention, the process that the coal raw material containing the low-rank coal is subjected to coking by using the stamp-charging coke oven is used, such that the problems of low existing stamp-charging coke oven utilization rate and excess coking industry production capacity are solved, and the problem that the application of the low-rank coal is limited due to no large-scale industrial equipment is solved.

Description

technical field [0001] The invention relates to a coking process, in particular to a coking process for coal raw materials containing low-rank coal, and belongs to the technical field of low-rank coal coking conversion. Background technique [0002] Coal is the main energy source in my country, accounting for about 70% of the primary energy structure. In the long process of geological evolution, the formation of coal is affected by many factors, resulting in various types of coal. According to the structure and composition, coal is divided into three categories: lignite, bituminous coal and anthracite. Bituminous coal is divided into low-metamorphic bituminous coal and medium-metamorphic bituminous coal. Low-metamorphic bituminous coal is also called sub-bituminous coal, which is collectively referred to as "low-rank coal" together with lignite. . Low-rank coal is the product of the initial stage of coalification. It has the characteristics of low carbon content, high mois...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

Application Information

Patent Timeline
no application Login to View More
Patent Type & Authority Patents(China)
IPC IPC(8): C10B53/08
Inventor 林科杜明来
Owner BEIJING SJ ENVIRONMENTAL PROTECTION & NEW MATERIAL CO LTD