A production method and air stone technology, applied in ceramic products, other household appliances, animal husbandry and other directions, can solve the problems of wear resistance, low strength, poor air permeability, etc., to increase the viewing degree, the production method is simple, and the The effect of overall strength
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment
[0046] Choose 180-1000 mesh white corundum sand powder;
[0047] Choose a mixture of high yellow dextrin water, ling clay powder, feldspar powder, talcum powder, and yellow dextrin powder as additives;
[0048] Among them, the mass proportion of white corundum sand powder is 70%, kaolin powder is 10%, feldspar powder is 7.65%, talc powder is 4%, and yellow dextrin powder is 8.35%;
[0049] Put the above-mentioned sand powder and additives into the mixer and stir and mix for 5 minutes to form a sand-stone mixture;
[0050] Put the above-mentioned sand and stone mixture into the selected steel mold, and use a press for extrusion molding, the pressure is 2T-500T, and the pressure is determined according to the size of the formed sand to form a sand-like body;
[0051]Dry the above-mentioned sand and gravel samples and put them into the kiln furnace. Raise the temperature of the kiln furnace to 1200°C and keep it for at least 2 hours. Drying ensures that the sand and gravel sampl...