Enrichment of calorific value of pyrite-type coal gangue and comprehensive utilization of iron
A technology of coal gangue and pyrite, which is applied in pyrite-type coal gangue heat value enrichment and comprehensive utilization of iron, can solve the problems of failure to propose flotation tailings destination and comprehensive utilization methods, and achieve recycling Improvement of means, improvement of chemical activity, and high dissolution rate
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment Construction
[0047] like figure 1 The shown pyrite briquette calorific value enrichment method and comprehensive utilization method of iron are prepared according to the following steps:
[0048] First, the pyrite coal gangue is pulverized to a certain fineness, and then sent to the acid leaching process to mix with the batching liquid, and sulfuric acid or hydrochloric acid is added to carry out acid leaching reaction under the condition of introducing an activator to make the silicate structure in the coal gangue. Under the action of sulfuric acid or hydrochloric acid, the aluminum element in it is converted into corresponding soluble salts and dissolved out, and the acid leaching solution and acid leaching residue are collected by filtration. The pyrite-type coal gangue refers to the coal gangue whose iron phase is pyrite (pyrite). Combined response mode.
[0049] The neutralization reaction:
[0050] Pulverize the coal gangue to 80-200 mesh, and then mix it with the acid leaching so...