Environment-friendly printing ink composition for PVC intaglio
An ink composition and an environmental protection technology are applied in the field of high temperature pigment discoloration environmental protection ink and its preparation, which can solve the problems of color change and chromatic aberration, affecting the printing quality of products, etc. Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0036] 1. The formula of the composition
[0037] 1. Prepare resin powder according to the mixing mass ratio, the mixing mass ratio is polyester powder: PVC powder: acrylic powder = 1:1:1;
[0038] 2. Prepare the solvent according to the mixing mass ratio, the mixing mass ratio is dimethyl succinate: methyl hydroxypropionate: methyl oleate: dimethyl glutarate = 10:2.5:0.5:3;
[0039] 3. The content of each component of the composition is prepared according to the mass percentage:
[0040]
[0041] 2. Preparation method
[0042] Add resin powder, solvents, additives, dispersants and fillers to the reaction kettle in sequence according to the mass percentage, and stir continuously at the same time to mix evenly; control the temperature of the reaction kettle at 45-60°C, add pigments to it, stir continuously, and mix Evenly; keep warm for 5-15 minutes, then add coupling agent, stir continuously, mix evenly; pack and seal for later use.
[0043] 3. Beneficial effects
[004...
Embodiment 2
[0046] 1. The formula of the composition
[0047] 1. Prepare resin powder according to the mixing mass ratio, the mixing mass ratio is polyester powder: PVC powder: acrylic powder = 1:1:1;
[0048] 2. Prepare the solvent according to the mixing mass ratio, the mixing mass ratio is dimethyl succinate: methyl hydroxypropionate: methyl oleate: dimethyl glutarate = 10:2.5:0.5:3;
[0049] 3. The content of each component of the composition is prepared according to the mass percentage:
[0050]
[0051] Two, preparation method is the same as embodiment 1
[0052] 3. Beneficial effects
[0053] The composition obtained in this embodiment, through testing, has no taste, does not change color in 16 minutes, has a grade 1 adhesion, no color difference, and a drying speed of 120 m / min.
Embodiment 3
[0055] 1. The formula of the composition
[0056] 1. Prepare resin powder according to the mixing mass ratio, the mixing mass ratio is polyester powder: PVC powder: acrylic powder = 1:1:1;
[0057] 2. Prepare the solvent according to the mixing mass ratio, the mixing mass ratio is dimethyl succinate: methyl hydroxypropionate: methyl oleate: dimethyl glutarate = 10:2.5:0.5:3;
[0058] 3. The content of each component of the composition is prepared according to the mass percentage:
[0059]
[0060]
[0061] Two, preparation method is the same as embodiment 1
[0062] 3. Beneficial effects
[0063]The composition obtained in this embodiment, through testing, has no taste, does not change color in 7 minutes, has grade 1 adhesion, no color difference, and a drying speed of 111 m / min.