A technology of LED ceiling lamps and LED lamp groups, applied in the direction of reflection/signal paint, reflectors, coatings, etc., can solve the effect of secondary optical processing of lamps is not very ideal, the mode of wireless connection control is not very simple, intelligent Stepless dimming is not very ideal, to achieve the effect of improving convenience, saving tediousness, and increasing aesthetics
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
preparation example Construction
[0048] A method for preparing a diffuse reflection coating for an LED ceiling lamp, the preparation steps of which are as follows: Pour polyvinyl alcohol into water at a temperature of 60-80°C, keep warm, stir well, so that the polyvinyl alcohol is fully dissolved and uniform; cool down to 30°C , add nano-magnesium oxide, stir evenly, add leveling agent and defoamer, stir evenly, then add nano-alumina, stir evenly, finally add barium sulfate, stir evenly, that is.
[0049] As a further optimization of this solution, the preparation method also includes adding rutile nano-titanium dioxide after adding nano-magnesia, stirring evenly, and then adding leveling agent and defoaming agent.
Embodiment 1
[0051] The raw materials that the present invention adopts are commercial gains, and wherein, rutile type nano-titanium dioxide is purchased from U.S. DuPont Company, and domestic current nano-titanium dioxide particle diameter is the lowest to be 100nm, defoamer can be selected Foamex822 defoamer, leveling agent can be purchased In Germany Merck MOK-2020.
[0052] In 1000g of water at 70°C, add 10g of polyvinyl alcohol, keep it warm for 90 minutes, stir it evenly with a high-speed mixer to fully dissolve it, cool the aqueous solution of vinyl alcohol to 30°C, add 205g of nano-magnesium oxide, stir evenly, add leveling agent and disinfectant 3g of each foaming agent, stirred evenly at high speed, then added 160g of nano-alumina, stirred evenly, finally added 310g of barium sulfate, and stirred evenly to obtain a diffuse reflective coating, wherein the barium sulfate particle size is 300nm, and the particle size of the nano-alumina The particle size of the nano magnesium oxide ...
Embodiment 2
[0056] The raw materials that the present invention adopts are commercial gains, and wherein, rutile type nano-titanium dioxide is purchased from U.S. DuPont Company, and domestic current nano-titanium dioxide particle diameter is the lowest to be 100nm, defoamer can be selected Foamex822 defoamer, leveling agent can be purchased In Germany Merck MOK-2020.
[0057] In 990g of water at 80°C, add 15g of polyvinyl alcohol, keep it warm for 90 minutes, stir evenly with a high-speed mixer to fully dissolve it, cool the aqueous solution of vinyl alcohol to 30°C, add 150g of nano-magnesia, stir evenly, add rutile nano-titanium dioxide, Stir evenly, add 4g of leveling agent and defoamer at the same time, stir evenly at high speed, then add 200g of nano-alumina, stir evenly, finally add 400g of barium sulfate, stir evenly, and obtain a diffuse reflective coating, wherein, the particle size of barium sulfate is The particle size of the nano-alumina is 13nm, the particle size of the nano...
PUM
Property | Measurement | Unit |
---|---|---|
particle diameter | aaaaa | aaaaa |
particle diameter | aaaaa | aaaaa |
particle diameter | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com