Rare-earth terbium complex, polyurethane foam doped with rare-earth terbium complex and application thereof
A technology of polyurethane foam and terbium complex, applied in the field of polyurethane foam and rare earth terbium complex, can solve the problems of high temperature resistance, unstable luminescence, weak rare earth ion terbium luminescence, etc. Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0046] The synthetic method of embodiment 1 ligand BAA:
[0047] The general synthetic route of ligand BAA is as follows:
[0048] The synthetic route of anthranilic acid:
[0049]
[0050] The synthetic route of ligand BAA:
[0051]
[0052] The specific preparation method of the ligand BAA comprises the following steps:
[0053] 1) Hydrolysis of methyl anthranilate to generate anthranilic acid: Weigh 30g (0.2mol) methyl anthranilate and 16g sodium hydroxide respectively, and pour the weighed anthranilic acid into a 200ml single-necked flask , then add 50ml of tetrahydrofuran to prepare a methyl anthranilate solution, then dissolve the weighed sodium hydroxide with 100ml of distilled water to prepare an aqueous sodium hydroxide solution, and add the aqueous sodium hydroxide solution to a single-necked flask with anthranilate Methyl formate solution was mixed. The mixed reaction solution was heated at 68° C., condensed to reflux, and reacted for 3 h. After the react...
Embodiment 2
[0056] Embodiment 2 A rare earth terbium complex, the rare earth terbium complex molecular formula is Tb(BAA) 3 2H 2 O, the structural formula is:
[0057]
[0058] Terbium complex Tb(BAA) 3 2H 2 The synthesis method of O:
[0059] Terbium complex Tb(BAA) 3 2H 2 The synthetic route of O is as follows:
[0060]
[0061] Terbium complex Tb(BAA) 3 2H 2 The specific preparation method of O comprises the following steps:
[0062] ① Weigh TbCl 3 ·6H 2 O (0.37g, 1mmol), dissolved in 20-30ml of absolute ethanol, was fully dissolved with the help of ultrasonic cleaner vibration, and the solution was pale white.
[0063] ②TbCl 3 ·6H 2 O and BAA coordinate according to the molar ratio of 1:3, so weigh BAA (0.78g, 3mmol), add it to a 100ml three-necked flask, and then add about 40ml of tetrahydrofuran to dissolve it. The color of the solution is clear and transparent.
[0064] ③ Pour the homogeneously dissolved solution in step ① into a three-necked flask, and the mixt...
Embodiment 3
[0072] Embodiment 3 doping terbium complex polyurethane foam:
[0073] The synthetic route of doped terbium complex polyurethane foam is as follows:
[0074]
[0075] The concrete preparation method of doped terbium complex polyurethane foam comprises the following steps:
[0076] 1) Preparation of polyols from ring-opened epoxidized soybean oil:
[0077] The epoxy groups in the ring-opened epoxy soybean oil and methanol were weighed at a molar ratio of 1:11, and 0.2% of the ring-opened epoxy soybean oil was added as a catalyst tetrafluoroboric acid to react to synthesize polyols. Weigh 9.5g (0.01mol) epoxy soybean oil, 14.08g (0.44mol) methanol and 0.047g tetrafluoroboric acid respectively. First add 14.08g of methanol into a round bottom flask, add 0.047g of tetrafluoroboric acid, then dropwise add epoxy soybean oil, and react at a reaction temperature of 65°C for 1.5 to 2 hours to obtain the reaction product polyol.
[0078] 2) Polyurethane foam
[0079] In this grou...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology