A sanitary napkin and active technology, applied in sanitary napkins, clothing, underwear, etc., can solve problems such as mutual interference, inability to combine sanitary napkins, and weak magnetic therapy effect, and achieve strong field effects, high field effects, and strong field effects Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0028] 1) Composition by weight of energy powder: 4.3 parts of diamond medicine stone, 3.8 parts of tourmaline, 0.38 parts of Hetian jade, 3.2 parts of coral stone, 1.35 parts of obsidian, 0.05 parts of citrine, 5 parts of medical stone, 3.9 parts of calcium gluconate, 0.5 part of Bianstone, 0.25 part of keel, weigh the materials and mix them thoroughly; use a grinder to grind at 545℃ to obtain energy powder of 2000 mesh to 6000 mesh;
[0029] 2) The energy powder of 2000 mesh to 6000 mesh is added with 14.5% ethanol of the total mass of the energy powder, then transferred to the nano grinder for grinding with 0.8-2.5 mm grinding media, dried and crushed to obtain nano-level energy powder;
[0030] 3) Weigh the polymer water-absorbing resin and the nano-level energy powder prepared in step 2) according to the ratio. The mass fraction of the energy powder in the polymer water-absorbing resin is 2.2%, and the two are evenly mixed to obtain the active polymer water-absorbing resin. Th...
Embodiment 2
[0032] 1) Composition by weight of energy powder: 4.4 parts of diamond medicine stone, 3.7 parts of tourmaline, 0.37 parts of Hetian jade, 3.1 parts of coral stone, 1.3 parts of obsidian, 0.04 parts of citrine, 4 parts of medical stone, 3.8 parts of calcium gluconate, 0.5 part of Bianstone and 0.22 part of keel Weigh the materials and mix them thoroughly; use a grinder to grind at a temperature of 540°C to obtain energy powder of 2000 mesh to 6000 mesh;
[0033] 2) Add 14% ethanol of the total mass of the energy powder to the energy powder of 2000 mesh to 6000 mesh, then transfer it to the nano grinder to grind it with a grinding medium of 0.8 mm to 2.5 mm, dry and crush to obtain nano energy powder;
[0034] 3) Weigh the polymer water-absorbing resin and the nano-level energy powder prepared in step 2) according to the ratio. The mass fraction of the energy powder in the polymer water-absorbing resin is 2.5%, and the two are mixed uniformly to obtain the active polymer water-absorb...
Embodiment 3
[0036] 1) Composition by weight of energy powder: 4.2 parts of diamond medicine stone, 3.6 parts of tourmaline, 0.36 parts of Hetian jade, 3.1 parts of coral stone, 1.33 parts of obsidian, 0.04 parts of citrine, 5 parts of medical stone, 3.9 parts of calcium gluconate, 0.5 part of Bianstone and 0.24 part of keel Weigh the materials and mix them thoroughly; use a grinder to grind at a temperature of 555°C to obtain energy powder of 2000 mesh to 6000 mesh;
[0037] 2) Add 13% ethanol of the total mass of the energy powder to the energy powder of 2000 mesh to 6000 mesh, then transfer it to the nano grinder to grind with the grinding medium of 0.8 mm to 2.5 mm, dry and crush to obtain nano-level energy powder;
[0038] 3) Weigh the polymer water-absorbing resin and the nano-level energy powder prepared in step 2) according to the ratio. The mass fraction of the energy powder in the polymer water-absorbing resin is 1.9%, and the two are evenly mixed to obtain the active polymer water-abs...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com