Mine sleeve repairing method

A casing and mining technology, which is applied in the field of mine casing repair, can solve the problems of high cost of pipe materials, heavy overall weight of the repaired pipe, and more cement for repairing, etc.

CN106639946AActive Publication Date: 2017-05-10CHNA ENERGY INVESTMENT CORP LTD +1
12 Cites 2 Cited by

Patent Information

Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Publication Date
2017-05-10

Smart Images

  • Figure 1
    Figure 1
Patent Text Reader

Abstract

The invention discloses a mine sleeve repairing method. The repairing method comprises the steps that (1) a repairing pipe with the appropriate length is selected according to a damage position range of the mine sleeve; (2) the head end of a drill rod and the head end of the repairing pipe are detachably connected , and a through hole in the extending direction of the drill rod is formed in the drill rod; (3) the tail end of the repairing pipe is inserted in a pipeline of the mine sleeve, the position of the repairing pipe is adjusted to enable the repairing pipe to cover the damage position range, and the outer wall of the tail end of the repairing pipe is fixedly connected with the inner wall of the mine sleeve; and (4) a reinforcement agent is injected through the through hole until a gap between the outer wall of the repairing pipe and the inner wall of the mine sleeve is fully filled with the reinforcement agent, and after the reinforcement agent is solidified, a reinforced layer is formed. By adopting the mine sleeve repairing method, the repairing cost of the mine sleeve is effectively reduced, the conduction period is shortened significantly, and meanwhile, a repairing mode and a well cementing mode are simplified.
Need to check novelty before this filing date? Find Prior Art

Description

technical field

[0001] The invention belongs to the field of mining machinery, in particular to a method for repairing casings used in mines. Background technique

[0002] With the development of drilling technology, various engineering holes have played an important role in the construction and production stages of coal mines. During the drilling construction operation, the mining casing is inserted after the engineering hole is drilled on the surface, and a cement sheath is injected between the outer wall of the mining casing and the inner wall of the engineering hole. However, as time goes by, due to wear and tear, poor management, and rock formation vibrations, etc., the engineering holes are more likely to be damaged, resulting in the rupture of the cement sheath and the mine casing, water leakage and other problems. brought certain hidden dangers.

[0003] In the prior art, the method of repairing the engineering hole is mostly used in the whole process of mine casin...

Examples

Embodiment Construction

[0018] The present invention will be described in detail below in conjunction with examples. Wherein the same components are denoted by the same reference numerals. It should be noted that the words "front", "rear", "left", "right", "upper" and "lower" used in the following description refer to the directions in the drawings, and the words "inner" and "outer ” refer to directions towards or away from the geometric center of a particular part, respectively.

[0019] figure 1 It is a structural schematic diagram of a mine casing repaired by the method of the embodiment of the present invention. Such as figure 1 As shown, the mine casing repair method provided by this preferred embodiment includes: step a): according to the damage position range 2 of the mine casing 1, a repair pipe 3 of an appropriate length is selected; step b): the drill pipe 4 is The head end is detachably connected to the head end of the repair pipe 3, wherein the drill rod 4 is provided with a through h...