A kind of leather and brown technology, which is applied in the field of brown leather preparation, can solve the problems of not being able to repair the damage of the leather surface well, the decline of the aesthetic effect, and the uneven color, so as to achieve good color fixing effect, more natural color, unique color effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0020] A method for preparing brown leather, the method comprising the following steps: step 1, changing the color of the leather embryo, processing the leather embryo through a surface grinder, the sandpaper used for processing is No. 120 sandpaper, and placing the processed leather embryo on the On the automatic skin spraying machine, the spray dyeing solution is used to evenly spray the skin embryos, and the skin embryos treated with the spray dyeing solution are placed in the washing machine. The skin embryo is processed for 20 minutes, then it is taken out and placed in the dryer to dry the skin embryo;
[0021] Step 2: Change the color of the finished product. Place the dried skin embryo in step 1 on the polishing machine, apply the mid-gloss shoe milk to the skin embryo, and apply the finishing aid A to the skin embryo. At this time, the polishing machine The rotation speed is 19 rpm, and finally the finishing aid B is applied to the leather embryo, and the rotation spe...
Embodiment 2
[0029] A method for preparing brown leather, the method comprising the following steps: step 1, changing the color of the leather embryo, processing the leather embryo through a surface grinder, the sandpaper used for processing is No. 120 sandpaper, and placing the processed leather embryo on the On the automatic skin spraying machine, the spray dyeing solution is used to evenly spray the skin embryos, and the skin embryos treated with the spray dyeing solution are placed in the washing machine. The skin embryo is processed for 15 minutes, then it is taken out and placed in the dryer to dry the skin embryo;
[0030] Step 2: Change the color of the finished product. Place the dried skin embryo in step 1 on the polishing machine, apply the mid-gloss shoe milk to the skin embryo, and apply the finishing aid A to the skin embryo. At this time, the polishing machine The rotation speed is 19 rpm, and finally the finishing aid B is applied to the leather embryo, and the rotation spe...
Embodiment 3
[0038] A method for preparing brown leather, the method comprising the following steps: step 1, changing the color of the leather embryo, processing the leather embryo through a surface grinder, the sandpaper used for processing is No. 120 sandpaper, and placing the processed leather embryo on the On the automatic skin spraying machine, the spray dyeing solution is used to evenly spray the skin embryos, and the skin embryos treated with the spray dyeing solution are placed in the washing machine. The skin embryo is processed for 30 minutes, then it is taken out and placed in the dryer to dry the skin embryo;
[0039] Step 2: Change the color of the finished product. Place the dried skin embryo in step 1 on the polishing machine, apply the mid-gloss shoe milk to the skin embryo, and apply the finishing aid A to the skin embryo. At this time, the polishing machine The rotation speed is 19 rpm, and finally the finishing aid B is applied to the leather embryo, and the rotation spe...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com