Method for improving insulation matching of high-voltage direct-current cable accessories based on nano-doping
A technology of high-voltage direct current and cable accessories, applied in the direction of organic insulators, rubber insulators, etc., to achieve the effects of low cost, suppression of charge accumulation, and simple process
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment Construction
[0021] The technical solution adopted by the present invention to solve its technical problems is:
[0022] 1. The ethylene-propylene rubber nanocomposite insulating material is prepared by melt-opening and hot-pressing molding. The open-rolling blending method can ensure that fillers, cross-linking agents and other additives are fully mixed in EPDM monomer; hot-pressing molding process can effectively Control the vulcanization temperature and thickness of the rubber sample, as well as the flatness of the surface. The specific preparation process of EPDM composite materials is as follows:
[0023] (1) Put the EPDM colloidal particles and filler in an oven at 60°C for 12 hours to remove the moisture in the particles.
[0024] (2) Preheat the rollers of the double-roll mill, keep the temperature of the rollers at about 160°C, and adjust the distance between the double rollers to a minimum of 2mm.
[0025] (3) Put EPDM between the double sticks and preheat for 10 minutes to ful...