An adhesive tape, an environmentally friendly technology, applied in the direction of adhesives, natural rubber adhesives, adhesive types, etc., can solve the problems of poor stability, many manufacturing processes, easy residual adhesive capacitors, etc., to achieve strong self-adhesiveness and stability, production The effect of less process and simple ingredients
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0032] like figure 1 As shown, the environmentally friendly cold-pressed adhesive tape provided by the present application is an adhesive layer 1 and an adhesive tape layer 2 from top to bottom. Wherein the component of adhesive layer 1 is mainly made up of latex, ammonia water, filler, antioxidant and mixing auxiliary agent, and the weight percent corresponding to each component is: the weight ratio that latex occupies is 55%, and the weight ratio that ammonia water occupies is 40%, the weight ratio of the filler is 0.3%, the weight ratio of the antioxidant is 0.3%, and the weight ratio of the mixing aid is 4.4%. The components are mixed and formulated according to the above method to form glue, and finally rolled The process is applied to the upper surface of the adhesive tape layer 2 to form the adhesive layer 1 . Further, the tape layer 2 includes a paper layer, and the paper layer is made of high-strength kraft paper, and the adhesive layer 1 and the tape layer 2 form th...
Embodiment 2
[0034] like figure 1 As shown, the environmentally friendly cold-pressed adhesive tape provided by the present application is an adhesive layer 1 and an adhesive tape layer 2 from top to bottom. Wherein the component of adhesive layer 1 is mainly made up of latex, ammonia water, filler, antioxidant and mixing auxiliary agent, and the weight percent corresponding to each component is: the weight ratio that latex occupies is 60%, and the weight ratio that ammonia water occupies is 37.5%, the weight ratio of the filler is 0.5%, the weight ratio of the antioxidant is 0.5%, the weight ratio of the mixing aid is 1.5%, and the components are mixed and formulated according to the above method to form glue, and finally rolled The process is applied to the upper surface of the adhesive tape layer 2 to form the adhesive layer 1 . Further, the tape layer 2 includes a paper layer, and the paper layer is made of high-strength kraft paper, and the adhesive layer 1 and the tape layer 2 form ...
Embodiment 3
[0036] like figure 1 As shown, the environmentally friendly cold-pressed adhesive tape provided by the present application is an adhesive layer 1 and an adhesive tape layer 2 from top to bottom. Wherein the components of the adhesive layer 1 are mainly composed of latex, ammonia water, filler, antioxidant and mixing aid, and the weight percentages corresponding to each component are: the weight ratio of the latex is 70%, and the weight ratio of the ammonia water is 27%, the weight ratio of the filler is 1.0%, the weight ratio of the antioxidant is 1.0%, the weight ratio of the mixing aid is 1.0%, and the components are mixed according to the above method to form glue, and finally rolled The process is applied to the upper surface of the tape layer 2 to form an adhesive layer 1. Further, the tape layer 2 includes a paper layer, and the paper layer is made of high-strength kraft paper. The adhesive layer 1 and the tape layer 2 form the environmentally friendly cold-pressed adhes...
PUM
| Property | Measurement | Unit |
|---|---|---|
| thickness | aaaaa | aaaaa |
| thickness | aaaaa | aaaaa |
| thickness | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
Login to View More 