Embodiment 1
[0020] Nano antibacterial material preparation comprises the following steps:
[0021] Step 1. Add 12 parts of TiO to 50 parts of deionized water 2 / Sb 2 S 3 Composite antibacterial colloid, 4 parts of methacrylic acid hydroxypropyl sulfonic acid, 2 parts of acrylic resin and 3 parts of polyoxyethylene ether, ultrasonic dispersion for 15 minutes, ultrasonic frequency 4000W, to form a stable aqueous solution with a particle size of 6.8nm;
[0022] Step 2. Add 18 parts of methyl cyclomethacrylate, 12 parts of butyl acrylate and 2 parts of pop emulsifier in sequence to the above aqueous solution at a temperature of 55°C and a stirring speed of 70 rpm / min. After fully stirring and mixing, Stand at room temperature for 2h;
[0023] Step 3. Add 3 parts of tartaric acid and 2 parts of propylene glycol methyl ether acetate to the above-mentioned organic aqueous solution after standing for pre-stirring for 20 minutes, and the stirring speed is 4500 rpm / min to obtain a mixed slurry; ...
Embodiment 2
[0032] Step 1. Add 8 parts of TiO to 50 parts of deionized water 2 / Sb 2 S 3Composite antibacterial colloid, 3 parts of methacrylic acid hydroxypropyl sulfonic acid, 2 parts of acrylic resin and 3 parts of polyoxyethylene ether, ultrasonic dispersion for 15 minutes, ultrasonic frequency 4000W, to form a stable aqueous solution with a particle size of 6.8nm;
[0033] All the other preparations are the same as in Example 1.
Embodiment 3
[0035] Step 1. Add 6 parts of TiO to 50 parts of deionized water 2 / Sb 2 S 3 Composite antibacterial colloid, 6 parts of methacrylic acid hydroxypropyl sulfonic acid, 2 parts of acrylic resin and 3 parts of polyoxyethylene ether, ultrasonic dispersion for 15 minutes, ultrasonic frequency 4000W, to form a stable aqueous solution with a particle size of 6.8nm;
[0036] All the other preparations are the same as in Example 1.