Embodiment 1
[0045] Embodiment 1; Take raw material by following components and weight: ammonium persulfate 8kg, potassium persulfate 7kg, potassium carbonate 15kg, sodium silicate 3kg, potassium oxalate 8kg, polyethylene glycol ether 4kg, sodium propoxide 3kg, potassium ethoxy acetate 7kg, decyldimethylamine 4kg, sodium methacrylate 2kg, laurylamine 11kg, sulfosuccinic acid 6kg, hydroxyethylethylenediamine 3kg, lipase 0.2kg.
[0046] According to the following steps, the raw materials in the above weight ratio are prepared into landfill leachate deodorization and degradation treatment agent composition:
[0047] 1. Stir 4kg of polyethylene glycol ether, 3kg of sodium propoxide, 4kg of decyldimethylamine and 11kg of laurylamine in a reaction kettle at a stirring speed of 120 rpm for 40 minutes until uniform to obtain a uniform paste shape.
[0048] 2. Mix 8kg of potassium oxalate, 2kg of sodium methacrylate, 6kg of sulfosuccinic acid and 3kg of hydroxyethylethylenediamine with a conical m...
Embodiment 2
[0052] Embodiment 2; Take raw material by following component and weight: ammonium persulfate 6kg, potassium persulfate 6kg, potassium carbonate 15kg, sodium silicate 2kg, potassium oxalate 10kg, polyethylene glycol ether 3kg, sodium propoxide 4kg, potassium ethoxy acetate 8kg, decyldimethylamine 3kg, sodium methacrylate 1kg, laurylamine 10kg, sulfosuccinic acid 5kg, hydroxyethylethylenediamine 4kg, lipase 0.3kg.
[0053] According to the following steps, the raw materials in the above weight ratio are prepared into landfill leachate deodorization and degradation treatment agent composition:
[0054] 1. Stir the above-mentioned polyethylene glycol ether, sodium propoxide, decyldimethylamine and laurylamine in a reaction kettle at a stirring speed of 150 rpm for 30 minutes until uniform to obtain a uniform paste.
[0055] 2. Mix the above-mentioned potassium oxalate, sodium methacrylate, sulfosuccinic acid and hydroxyethylethylenediamine with a conical mixing mixer until unifor...
Embodiment 3
[0059] Embodiment 3; Take raw material by following component and weight: ammonium persulfate 9kg, potassium persulfate 4kg, potassium carbonate 11kg, sodium silicate 4kg, potassium oxalate 9kg, polyethylene glycol ether 5kg, sodium propoxide 2kg, potassium ethoxy acetate 9kg, decyldimethylamine 5kg, sodium methacrylate 3kg, laurylamine 8kg, sulfosuccinic acid 7kg, hydroxyethylethylenediamine 2kg, lipase 0.15kg.
[0060] According to the following steps, the raw materials in the above weight ratio are prepared into landfill leachate deodorization and degradation treatment agent composition:
[0061] 1. Stir the above polyethylene glycol ether, sodium propoxide, decyldimethylamine and laurylamine in a reaction kettle at a stirring speed of 120 rpm for 40 minutes until uniform to obtain a uniform paste.
[0062] 2. Mix the above-mentioned potassium oxalate, sodium methacrylate, sulfosuccinic acid and hydroxyethylethylenediamine with a conical mixing mixer until uniform, the stir...
PUM
Property | Measurement | Unit |
---|---|---|
density | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com