A production method and fabric technology, applied in the direction of fabric, fabric surface trimming, heating/cooling fabric, etc., can solve the problems of fabric deformation, troublesome operation, low efficiency, etc., and achieve non-deformation, good imitation effect, and good wearing comfort Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0037] In this embodiment, a method for making an old-fashioned effect fabric includes the following steps:
[0038] (1) Perform low-temperature bulking agent and permanent antistatic finishing on conventional warp and weft yarns used for weaving: add water and silicone softener polyester fluffy softener SR 3g / L (from Xian, Dongguan City) to the package dyeing machine Bridge Auxiliary Industry Co., Ltd.), antistatic finishing agent TG-01A 2g / L (from Huntsman Chemical), run at 45°C for 25min, drain, dehydrate, and dry, and prepare for use;
[0039] (2) Preparation of composite yarn: Two or more of the conventional yarn obtained in step (1), low-temperature hot-melt yarn at 80-150°C, and low-temperature water-soluble yarn at 20-90°C are parallel-twisted to obtain 50D- 200D functional composite yarn;
[0040] Wherein, the conventional yarn is co-twisted with 80-130°C low-temperature heat-melt yarn to form the first composite yarn; the conventional yarn is co-twisted with 20-90°C...
Embodiment 2
[0049]In this embodiment, a method for making an old-fashioned effect fabric includes the following steps:
[0050] (1) Perform low-temperature fluffing agent finishing on conventional warp and weft yarns used for weaving: in the package dyeing machine, add water, and silicone softener polyester fluffy softener SR 3g / L (from Dongguan Xianqiao Auxiliary Industry Co., Ltd. company), run at 45°C for 25 minutes, drain, dehydrate, and dry, and prepare for use;
[0051] (2) Composite yarn preparation: similar to Example 1;
[0052] (3) Gray fabric pattern design: similar to Example 1;
[0053] (4) weaving: according to the gray cloth pattern design of step (3), warp and weft interweaving is carried out to each yarn to obtain gray cloth;
[0054] (5) Shaping: at a temperature of 145°C and a pressure of 5kg / cm 2 Carry out ironing and shaping to the gray cloth under certain conditions, and the ironing and shaping time is 20-100s;
[0055] (6) Fabrication of woven labels: Cut the sh...
Embodiment 3
[0060] In this embodiment, a method for making an old-fashioned effect fabric includes the following steps:
[0061] (1) The conventional warp and weft yarns used for weaving are not treated with low-temperature bulking agents;
[0062] (2) Composite yarn preparation: similar to Example 1;
[0063] (3) Gray fabric pattern design: similar to Example 1;
[0064] (4) weaving: according to the gray cloth pattern design of step (3), warp and weft interweaving is carried out to each yarn to obtain gray cloth;
[0065] (5) Shaping: at a temperature of 145°C and a pressure of 5kg / cm 2 Carry out ironing and shaping to the gray cloth under certain conditions, and the ironing and shaping time is 20-100s;
[0066] (6) Fabrication of woven labels: Cut the shaped gray cloth according to conventional methods to make woven labels (including strips and trademark products). Specifically, according to the distribution of hot-melt yarns in the gray cloth, hot-cut, cold-cut, Cutting by one or ...