Recyclable mildewproof powder for glass and preparation method of recyclable mildewproof powder
A mildew and glass technology, applied in powder coatings, anti-corrosion coatings, coatings, etc., can solve problems such as economic loss, impact on the final use of glass, corrosion, etc., and achieve the effects of avoiding mildew, improving mildew resistance and economic benefits
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0020] A recyclable glass mold-proof powder, its composition by weight: 15 parts of polyester resin, 15 parts of polyethylene, 25 parts of water glass, 50 parts of hydrochloric acid, 15 parts of boric anhydride, 1 part of sorbic acid, ethylene glycol 3 parts of acid, 2 parts of copper chloride, appropriate amount of water.
[0021] A kind of preparation method of recyclable glass mold proof powder comprises the following steps:
[0022] a. Pulverization: After weighing the raw materials according to the proportion, put the skeleton isolation base powder, boric anhydride, sorbic acid, benzoic acid, oxalic acid and copper chloride into the ball mill respectively for ball milling. The rotating speed of a ball mill is 1050rpm. The mesh number is 600 mesh;
[0023] b. Dissolution and reaction: add hydrochloric acid and the skeleton isolation base powder obtained in step a, boric anhydride, sorbic acid, benzoic acid, oxalic acid and copper chloride to an appropriate amount of water...
Embodiment 2
[0026] A kind of recyclable glass mildew-proof powder, its composition by weight: 20 parts of polyethylene, 15 parts of polypropylene, 20 parts of water glass, 40 parts of hydrochloric acid, 25 parts of boric anhydride, 3 parts of sorbic acid, oxalic acid 2 parts, 3 parts of copper chloride, appropriate amount of water.
[0027] A kind of preparation method of recyclable glass mold proof powder comprises the following steps:
[0028] a. Pulverization: After weighing the raw materials according to the proportion, put the skeleton isolation base powder, boric anhydride, sorbic acid, benzoic acid, oxalic acid and copper chloride into the ball mill respectively for ball milling. The rotating speed of a ball mill is 1000rpm. The mesh number is 750 mesh;
[0029] b. Dissolution and reaction: add hydrochloric acid and the skeleton isolation base powder obtained in step a, boric anhydride, sorbic acid, benzoic acid, oxalic acid and copper chloride to an appropriate amount of water, a...
Embodiment 3
[0032] A kind of recyclable glass anti-mold powder, its composition by weight: 25 parts of polypropylene, 15 parts of polymethyl methacrylate, 25 parts of water glass, 55 parts of hydrochloric acid, 10 parts of boric anhydride, 4 parts of sorbic acid , 5 parts of oxalic acid, 1 part of copper chloride, and appropriate amount of water.
[0033] A kind of preparation method of recyclable glass mold proof powder comprises the following steps:
[0034] a. Pulverization: After weighing the raw materials according to the proportion, put the skeleton isolation base powder, boric anhydride, sorbic acid, benzoic acid, oxalic acid and copper chloride into the ball mill respectively for ball milling. The rotating speed of a ball mill is 100rpm. The mesh number is 900 mesh;
[0035] b. Dissolution and reaction: add hydrochloric acid and the skeleton isolation base powder obtained in step a, boric anhydride, sorbic acid, benzoic acid, oxalic acid and copper chloride to an appropriate amou...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com